General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.6 g/cm³ Show Supplier Material materials with Density of 2.6 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1000.0 °C | 4.8E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.8E-6 1/K | |
Max service temperature | 1800 °C Show Supplier Material materials with Max service temperature of 1800 °C | in inert gas | |
Max service temperature, long | 1600 °C Show Supplier Material materials with Max service temperature, long of 1600 °C | in air | |
Thermal conductivity | 23.0 °C | 23 W/(m·K) Show Supplier Material materials with Thermal conductivity of 23 W/(m·K) | |
Thermal shock parameter R1 | 69 °C Show Supplier Material materials with Thermal shock parameter R1 of 69 °C | ||
Thermal shock parameter R2 | 1597 W/m Show Supplier Material materials with Thermal shock parameter R2 of 1597 W/m |