General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 3.26 g/cm³ Show Supplier Material materials with Density of 3.26 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 300 GPa Show Supplier Material materials with Elastic modulus of 300 GPa |
Flexural strength | 23.0 °C | 970 MPa Show Supplier Material materials with Flexural strength of 970 MPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 6.2 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6.2 MPa·√m |
Poisson's ratio | 23.0 °C | 0.26 [-] Show Supplier Material materials with Poisson's ratio of 0.26 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1.4E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.4E-6 1/K | |
1000.0 °C | 3.2E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.2E-6 1/K | ||
Max service temperature | 1400 °C Show Supplier Material materials with Max service temperature of 1400 °C | in inert gas | |
Max service temperature, long | 1200 °C Show Supplier Material materials with Max service temperature, long of 1200 °C | in air | |
Thermal conductivity | 23.0 °C | 24 W/(m·K) Show Supplier Material materials with Thermal conductivity of 24 W/(m·K) | |
Thermal shock parameter R1 | 748 °C Show Supplier Material materials with Thermal shock parameter R1 of 748 °C | ||
Thermal shock parameter R2 | 17945 W/m Show Supplier Material materials with Thermal shock parameter R2 of 17945 W/m |