General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 3.55 g/cm³ Show Supplier Material materials with Density of 3.55 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 310 GPa Show Supplier Material materials with Elastic modulus of 310 GPa |
Flexural strength | 23.0 °C | 720 MPa Show Supplier Material materials with Flexural strength of 720 MPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 6 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6 MPa·√m |
Poisson's ratio | 23.0 °C | 0.26 [-] Show Supplier Material materials with Poisson's ratio of 0.26 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1.9E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.9E-6 1/K | |
Max service temperature | 1000 °C Show Supplier Material materials with Max service temperature of 1000 °C | in inert gas | |
Max service temperature, long | 800 °C Show Supplier Material materials with Max service temperature, long of 800 °C | in air | |
Thermal conductivity | 23.0 °C | 21 W/(m·K) Show Supplier Material materials with Thermal conductivity of 21 W/(m·K) |