General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 3.17 g/cm³ Show Supplier Material materials with Density of 3.17 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 420 GPa Show Supplier Material materials with Elastic modulus of 420 GPa |
Flexural strength | 23.0 °C | 420 MPa Show Supplier Material materials with Flexural strength of 420 MPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 2.7 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 2.7 MPa·√m |
Poisson's ratio | 23.0 °C | 0.15 [-] Show Supplier Material materials with Poisson's ratio of 0.15 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 2.5E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5E-6 1/K | |
1000.0 °C | 4.5E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.5E-6 1/K | ||
Max service temperature | 1900 °C Show Supplier Material materials with Max service temperature of 1900 °C | in inert gas | |
Max service temperature, long | 1600 °C Show Supplier Material materials with Max service temperature, long of 1600 °C | in air | |
Thermal conductivity | 23.0 °C | 100 W/(m·K) Show Supplier Material materials with Thermal conductivity of 100 W/(m·K) | |
Thermal shock parameter R1 | 189 °C Show Supplier Material materials with Thermal shock parameter R1 of 189 °C | ||
Thermal shock parameter R2 | 18889 W/m Show Supplier Material materials with Thermal shock parameter R2 of 18889 W/m |