General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 4.4 g/cm³ Show Supplier Material materials with Density of 4.4 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 540 GPa Show Supplier Material materials with Elastic modulus of 540 GPa |
Flexural strength | 23.0 °C | 480 MPa Show Supplier Material materials with Flexural strength of 480 MPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 5 MPa·√m |
Poisson's ratio | 23.0 °C | 0.33 [-] Show Supplier Material materials with Poisson's ratio of 0.33 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 4.6E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.6E-6 1/K | |
1000.0 °C | 7.6E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.6E-6 1/K | ||
Max service temperature | 2000 °C Show Supplier Material materials with Max service temperature of 2000 °C | in inert gas | |
Max service temperature, long | 600 °C Show Supplier Material materials with Max service temperature, long of 600 °C | in air | |
Thermal conductivity | 23.0 °C | 24 W/(m·K) Show Supplier Material materials with Thermal conductivity of 24 W/(m·K) | |
Thermal shock parameter R1 | 78 °C Show Supplier Material materials with Thermal shock parameter R1 of 78 °C | ||
Thermal shock parameter R2 | 1881 W/m Show Supplier Material materials with Thermal shock parameter R2 of 1881 W/m |