General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 4.9 g/cm³ Show Supplier Material materials with Density of 4.9 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 495 GPa Show Supplier Material materials with Elastic modulus of 495 GPa |
Flexural strength | 23.0 °C | 220 MPa Show Supplier Material materials with Flexural strength of 220 MPa |
Poisson's ratio | 23.0 °C | 0.19 [-] Show Supplier Material materials with Poisson's ratio of 0.19 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1000.0 °C | 7.4E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.4E-6 1/K | |
Max service temperature | 2000 °C Show Supplier Material materials with Max service temperature of 2000 °C | in inert gas | |
Max service temperature, long | 600 °C Show Supplier Material materials with Max service temperature, long of 600 °C | in air | |
Thermal conductivity | 23.0 °C | 24 W/(m·K) Show Supplier Material materials with Thermal conductivity of 24 W/(m·K) | |
Thermal shock parameter R1 | 49 °C Show Supplier Material materials with Thermal shock parameter R1 of 49 °C | ||
Thermal shock parameter R2 | 1168 W/m Show Supplier Material materials with Thermal shock parameter R2 of 1168 W/m |