Properties

General

Density ρ

6.1 g/cm³ at 20 °C

Mechanical

Elastic modulus E

490 GPa at 20 °C

Fracture toughness KIC

4 MPa·√m at 20 °C

Poisson's ratio ν

0.3 [-] at 20 °C

Thermal

Coefficient of thermal expansion α

5.9E-6 1/K at 20 °C

Show chart

Max service temperature Tmax

2200 °C

in inert gas

Max service temperature, long Tmaxlong

500 °C

in air

Thermal conductivity λ

23 W/(m·K) at 20 °C

This material data has been provided by FCT Ingenieurkeramik.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.