Properties

General

Density ρ

6.05 g/cm³ at 20 °C

Mechanical

Elastic modulus E

200 GPa at 20 °C

Flexural strength σbend

900 MPa at 20 °C

Fracture toughness KIC

10 MPa·√m at 20 °C

Poisson's ratio ν

0.3 [-] at 20 °C

Thermal

Coefficient of thermal expansion α

8E-6 1/K at 20 °C

Show chart

Max service temperature Tmax

800 °C

in inert gas

Max service temperature, long Tmaxlong

800 °C

in air

Thermal conductivity λ

2 W/(m·K) at 20 °C

Thermal shock parameter R1 R1

286 °C

Thermal shock parameter R2 R2

573 W/m