EN CuZn37Pb0,5 Leaded Brass

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Fitco.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Supplier Material materials with Aluminium of 0.05 %

Copper

62 - 64 %

Show Supplier Material materials with Copper of 62 - 64 %

Iron

0.1 %

Show Supplier Material materials with Iron of 0.1 %

Lead

0.1 - 0.8 %

Show Supplier Material materials with Lead of 0.1 - 0.8 %

Nickel

0.3 %

Show Supplier Material materials with Nickel of 0.3 %

Tin

0.2 %

Show Supplier Material materials with Tin of 0.2 %

Zinc

Balance, REM