PropertyTemperatureValue

Density

23.0 °C

17.3 - 17.7 g/cm³

Show Supplier Material materials with Density of 17.3 - 17.7 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

2 - 8 %

Show Supplier Material materials with Elongation of 2 - 8 %

Hardness, Vickers, 10

23.0 °C

280 - 330 [-]

Show Supplier Material materials with Hardness, Vickers, 10 of 280 - 330 [-]

Tensile strength

23.0 °C

580 - 650 MPa

Show Supplier Material materials with Tensile strength of 580 - 650 MPa

Chemical properties

PropertyValueComment

Aluminium

2E-3 %

Show Supplier Material materials with Aluminium of 2E-3 %

Max.

Arsenic

2E-3 %

Show Supplier Material materials with Arsenic of 2E-3 %

Max.

Calcium

2E-3 %

Show Supplier Material materials with Calcium of 2E-3 %

Max.

Carbon

5E-3 %

Show Supplier Material materials with Carbon of 5E-3 %

Max.

Chromium

2E-3 %

Show Supplier Material materials with Chromium of 2E-3 %

Max.

Cobalt

3E-3 %

Show Supplier Material materials with Cobalt of 3E-3 %

Max.

Copper

1E-3 %

Show Supplier Material materials with Copper of 1E-3 %

Max.

Magnesium

2E-3 %

Show Supplier Material materials with Magnesium of 2E-3 %

Max.

Molybdenum

5E-3 %

Show Supplier Material materials with Molybdenum of 5E-3 %

Max.

Other

7.5 %

Show Supplier Material materials with Other of 7.5 %

Ni+Fe

Potassium

1E-3 %

Show Supplier Material materials with Potassium of 1E-3 %

Max.

Silicon

3E-3 %

Show Supplier Material materials with Silicon of 3E-3 %

Max.

Sodium

2E-3 %

Show Supplier Material materials with Sodium of 2E-3 %

Max.

Sulfur

2E-3 %

Show Supplier Material materials with Sulfur of 2E-3 %

Max.

Tungsten

balance

Technological properties

Property
Application areas

Material to balance rotating systems (aviation, radar, crankshafts etc.); Radiation protection material (Shielding parts for medical diagnostic and radiation therapy); Material for tool holders and high speed spindles; Upsetting tools; Moulds for aluminium, magnesium, zinc and copper high pressure die casting