Description

Notwithstanding the dangers that slightly radioactive electrodes may pose, many welders in Europe and Asia continue to swear by “their red” WTh20. Up to 4 percent by weight of thorium dioxide is added to alloys of the WTh type during production. Ignitability increases with a higher oxide content compared to pure tungsten. Thoriated tungsten is used wherever a stable electron exit is essential: in plasma spraying, electron beam sources and also welding. The electrode responds “good naturedly” to high amperages. But it must be handled with special caution: Vapours or fine dust produced during welding or while resharpening the electrode tip can cause health problems in the body. Implementing suitable safety measures (extraction) is very important in this case. Our company is Europe’s sole manufacturer authorised for tungsten-thorium production, which is also why we offer the only WTh electrodes that are 100% compliant with German quality standards.

This material data has been provided by Gesellschaft für Wolfram Industrie GmbH .

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

18 - 18.9 g/cm³

Show Supplier Material materials with Density of 18 - 18.9 g/cm³

(depends on the forming degree)

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

6 %

Show Supplier Material materials with Elongation of 6 %

Max.

Tensile strength

23.0 °C

1300 - 2200 MPa

Show Supplier Material materials with Tensile strength of 1300 - 2200 MPa

at diameter 1.0–3.2 mm

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

4.5E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 4.5E-6 1/K

at 0–100°C

Thermal conductivity

23.0 °C

174 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 174 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

27.0 °C

5.65E-6 Ω·m

Show Supplier Material materials with Electrical resistivity of 5.65E-6 Ω·m

227.0 °C

1.06E-5 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.06E-5 Ω·m

727.0 °C

2.49E-5 Ω·m

Show Supplier Material materials with Electrical resistivity of 2.49E-5 Ω·m

1227.0 °C

4.04E-5 Ω·m

Show Supplier Material materials with Electrical resistivity of 4.04E-5 Ω·m

1727.0 °C

5.67E-5 Ω·m

Show Supplier Material materials with Electrical resistivity of 5.67E-5 Ω·m

2227.0 °C

7.39E-5 Ω·m

Show Supplier Material materials with Electrical resistivity of 7.39E-5 Ω·m

2727.0 °C

9.2E-5 Ω·m

Show Supplier Material materials with Electrical resistivity of 9.2E-5 Ω·m

3227.0 °C

1.11E-4 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.11E-4 Ω·m

Chemical properties

PropertyValueComment

Aluminium

2E-3 %

Show Supplier Material materials with Aluminium of 2E-3 %

Max.

Arsenic

2E-3 %

Show Supplier Material materials with Arsenic of 2E-3 %

Max.

Calcium

2E-3 %

Show Supplier Material materials with Calcium of 2E-3 %

Max.

Carbon

5E-3 %

Show Supplier Material materials with Carbon of 5E-3 %

Max.

Chromium

2E-3 %

Show Supplier Material materials with Chromium of 2E-3 %

Max.

Cobalt

3E-3 %

Show Supplier Material materials with Cobalt of 3E-3 %

Max.

Copper

1E-3 %

Show Supplier Material materials with Copper of 1E-3 %

Max.

Iron

3E-3 %

Show Supplier Material materials with Iron of 3E-3 %

Max.

Magnesium

2E-3 %

Show Supplier Material materials with Magnesium of 2E-3 %

Max.

Molybdenum

5E-3 %

Show Supplier Material materials with Molybdenum of 5E-3 %

Max.

Nickel

2E-3 %

Show Supplier Material materials with Nickel of 2E-3 %

Max.

Potassium

1E-3 %

Show Supplier Material materials with Potassium of 1E-3 %

Max.

Silicon

3E-3 %

Show Supplier Material materials with Silicon of 3E-3 %

Max.

Sodium

2E-3 %

Show Supplier Material materials with Sodium of 2E-3 %

Max.

Sulfur

2E-3 %

Show Supplier Material materials with Sulfur of 2E-3 %

Max.

Thorium

1.8 - 2.2 %

Show Supplier Material materials with Thorium of 1.8 - 2.2 %

as ThO2

Tungsten

balance

Technological properties

Property
Application areas

Non melting electrode for TIG welding; Electrodes for lightning; Electrodes for plasma cutting and welding and thermal spraying; Cathodes for electronic tubes, wires in different electric applications

Processing history

Heat treatment: annealed, unannealed

Surface Finish

ground, drawn (black/cleaned), hammered