LDPE GM7

Alternative and trade names
GM7
Want to keep this datasheet? Save it now in your required format

Description

Low Density Polyethylene (LDPE) with moisture absorption of 0.0043% (100°C - 1hr)

This material data has been provided by Green Minds Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.96 g/cm³

Show Supplier Material materials with Density of 0.96 g/cm³

ASTM D793

Moisture absorption

23.0 °C

4.3E-3 %

Show Supplier Material materials with Moisture absorption of 4.3E-3 %

ASTM D6982, 100°C - 1hr

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1000 %

Show Supplier Material materials with Elongation of 1000 %

min., ASTM D638

Tensile strength

23.0 °C

17.16 MPa

Show Supplier Material materials with Tensile strength of 17.16 MPa

ASTM D638

Rheological Properties

PropertyValueComment

Melt mass-flow rate

37 g/10min

Show Supplier Material materials with Melt mass-flow rate of 37 g/10min

ASTM D1238, 190°C/2.16Kg

Technological properties

Property
Application areas

Irrigation Hoses, Electric Hoses - Film Grade

Color

Milky