Tungsten Carbide Cobalt, Powder Grade F

Want to keep this datasheet? Save it now in your required format

Description

The zinc process is an environmentally friendly way to reclaim tungsten carbide-cobalt from used hard materials, such as cutting inserts, milling tools or other hard material compacts. This secondary raw material stream provides cost-effective and reliable high quality tungsten carbide powder grades. GTP's subsidiary Tikomet has consistently made improvements to the zinc reclaim process for more than two decades. Switch to an environmentally friendly raw material source and rely on our recycling experience.

This material data has been provided by Global Tungsten & Powders Corp..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

14.49 g/cm³

Show Supplier Material materials with Density of 14.49 g/cm³

Grain size

0.8 - 1.3 μm

Show Supplier Material materials with Grain size of 0.8 - 1.3 μm

tungsten carbide grain size

Particle size D90

16 μm

Show Supplier Material materials with Particle size D90 of 16 μm

max

Mechanical

PropertyTemperatureValue

Hardness, Vickers, 30

23.0 °C

1560 [-]

Show Supplier Material materials with Hardness, Vickers, 30 of 1560 [-]

Magnetic

PropertyTemperatureValue

Coercive force

23.0 °C

19104 A/m

Show Supplier Material materials with Coercive force of 19104 A/m

Chemical properties

PropertyValueComment

Aluminium

0.02 %

Show Supplier Material materials with Aluminium of 0.02 %

max

Carbon

as WC balance

Chromium

0.6 %

Show Supplier Material materials with Chromium of 0.6 %

max

Cobalt

8 - 12 %

Show Supplier Material materials with Cobalt of 8 - 12 %

Copper

0.02 %

Show Supplier Material materials with Copper of 0.02 %

max

Iron

0.3 %

Show Supplier Material materials with Iron of 0.3 %

max

Nickel

0.1 %

Show Supplier Material materials with Nickel of 0.1 %

max

Niobium

0.1 %

Show Supplier Material materials with Niobium of 0.1 %

max

Oxygen

0.3 %

Show Supplier Material materials with Oxygen of 0.3 %

max

Tantalum

0.1 %

Show Supplier Material materials with Tantalum of 0.1 %

max

Titanium

0.1 %

Show Supplier Material materials with Titanium of 0.1 %

max

Tungsten

as WC balance

Vanadium

0.2 %

Show Supplier Material materials with Vanadium of 0.2 %

max

Zinc

5E-3 %

Show Supplier Material materials with Zinc of 5E-3 %

max

Technological properties

Property
Application areas

Powder grade F was developed for use in a wide range of tooling products, such as hardmetal rods, indexable inserts, woodworking tools and wear parts.

Other

Grade F powder exhibits a unifrom WC grain size distribution with evenly distributed WC and Cobalt particles. Thanks to the fine particle size of the powder, milling characteristics are great and comparable to virgin WC-Co powders.