ALFACOM® 40CRL

Want to keep this datasheet? Save it now in your required format

Description

Recycled glass fiber reinforced PP, chemically coupled and 100% recycled compound.

This material data has been provided by Green World Compounding.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Recycled Content

100 %

Show Supplier Material materials with Recycled Content of 100 %

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

5.98 - 7.02 GPa

Show Supplier Material materials with Elastic modulus of 5.98 - 7.02 GPa

ISO 527-1,-2

Elongation

23.0 °C

3 - 6 %

Show Supplier Material materials with Elongation of 3 - 6 %

Flexural modulus

23.0 °C

5.7 - 6.7 GPa

Show Supplier Material materials with Flexural modulus of 5.7 - 6.7 GPa

Flexural yield strength

23.0 °C

105 - 120 MPa

Show Supplier Material materials with Flexural yield strength of 105 - 120 MPa

ISO 178

Impact strength, Charpy unnotched

23.0 °C

30 - 40 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 30 - 40 kJ/m²

ISO 179

Yield strength

23.0 °C

65 - 80 MPa

Show Supplier Material materials with Yield strength of 65 - 80 MPa

Rheological Properties

PropertyValueComment

Melt mass-flow rate

3 - 6 g/10min

Show Supplier Material materials with Melt mass-flow rate of 3 - 6 g/10min

230°C/2.16kg, ISO 1133

Technological properties

Property
Application areas

Automotive, household appliances, furniture, construction, fitting, industrial injection. Design of products tailored to customer requirements.

Color

Black

Fillers

37-43% Glass Fiber