96% Alumina

Want to keep this datasheet? Save it now in your required format

Description

96 Alumina a high purity alumina ceramic with excellent mechanical, electrical, thermal, and chemical properties, benefiting from the following features:


  • Superior electrical properties
  • High mechanical strength and wear resistance
  • Moly-manganese metallized
  • Chemical and corrosion resistance
  • Excellent dielectric properties
  • Dense, non porous and vacuum tight
  • This material data has been provided by Innovacera.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    3.7 g/cm³

    Show Supplier Material materials with Density of 3.7 g/cm³

    Mechanical

    PropertyTemperatureValue

    Compressive strength

    23.0 °C

    2068 MPa

    Show Supplier Material materials with Compressive strength of 2068 MPa

    Elastic modulus

    23.0 °C

    280 - 320 GPa

    Show Supplier Material materials with Elastic modulus of 280 - 320 GPa

    Flexural strength

    23.0 °C

    320 MPa

    Show Supplier Material materials with Flexural strength of 320 MPa

    Hardness, Vickers

    23.0 °C

    1377 [-]

    Show Supplier Material materials with Hardness, Vickers of 1377 [-]

    Plane-Strain Fracture Toughnes

    23.0 °C

    4 - 5 MPa·√m

    Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 - 5 MPa·√m

    Poisson's ratio

    23.0 °C

    0.22 - 0.23 [-]

    Show Supplier Material materials with Poisson's ratio of 0.22 - 0.23 [-]

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    23.0 °C

    8.2E-6 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 8.2E-6 1/K

    Specific heat capacity

    23.0 °C

    780 J/(kg·K)

    Show Supplier Material materials with Specific heat capacity of 780 J/(kg·K)

    Thermal conductivity

    23.0 °C

    24 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 24 W/(m·K)

    Thermal shock parameter R2

    200 W/m

    Show Supplier Material materials with Thermal shock parameter R2 of 200 W/m

    Electrical

    PropertyTemperatureValue

    Dielectric constant

    23.0 °C

    9 [-]

    Show Supplier Material materials with Dielectric constant of 9 [-]

    Dielectric strength

    23.0 °C

    15 kV/mm

    Show Supplier Material materials with Dielectric strength of 15 kV/mm

    Electrical resistivity

    23.0 °C

    1.00E+16 Ω·m

    Show Supplier Material materials with Electrical resistivity of 1.00E+16 Ω·m

    Loss tangent

    23.0 °C

    4E-4 [-]

    Show Supplier Material materials with Loss tangent of 4E-4 [-]

    Technological properties

    Property
    Application areas

    Wear ceramic parts: Ceramic Nozzles, Ceramic, Sprayers Cyclones, Homogenising devices, Ceramic Linings, Milling Systems, Ceramic Thread guides - Precision components: Ceramic Measuring Components, Ceramic Control systems, (Micro) dosing valves, Electronic Components (electrical inductors, switches), Mechatronics, Optical applications - Machine-construction: Positioning Guide parts, Coatings, Transport ceramic rollers, Ceramic Dies, Textile machine parts, Furnace parts - Rotating equipment: Ceramic Sliding Bearings, Ceramic Ball bearings, Mechanical seals, Ceramic Plungers, Ceramic Valves / fittings, Dosing components - Cutting & moulding: Ceramic knives, Metal-forming tools, Seaming rolls, Ceramic Punches, Drawing dies

    Processing methods

    Ceramic Injection Molding, Low Pressure Injection Molding, Cold Isostatic Press, Dry Press, Tape Casting, Precision Machining Processing