The material of the ceramic reflector is 99% Al₂O₃. Its green body is fired at a suitable temperature to retain the proper porosity and strength. The surface of the ceramic reflector is coated with a high reflectivity ceramic glaze, so compared with the gold-plated reflector, it has long service life and diffuse reflection.

This material data has been provided by Innovacera.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

3.1 g/cm³

Show Supplier Material materials with Density of 3.1 g/cm³

Mechanical

PropertyTemperatureValue

Flexural strength

23.0 °C

170 MPa

Show Supplier Material materials with Flexural strength of 170 MPa

Hardness, Vickers

23.0 °C

0 [-]

Show Supplier Material materials with Hardness, Vickers of 0 [-]

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

7.9E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 7.9E-6 1/K

Technological properties

Property
Application areas

Wear ceramic parts: Ceramic Nozzles, Ceramic, Sprayers Cyclones, Homogenising devices, Ceramic Linings, Milling Systems, Ceramic Thread guides - Precision components: Ceramic Measuring Components, Ceramic Control systems, (Micro) dosing valves, Electronic Components, Mechatronics, Optical applications - Machine-construction: Positioning Guide parts, Coatings, Transport ceramic rollers, Ceramic Dies, Textile machine parts, Furnace parts - Rotating equipment: Ceramic Sliding Bearings, Ceramic Ball bearings, Mechanical seals, Ceramic Plungers, Ceramic Valves / fittings, Dosing components - Cutting & moulding: Ceramic knives, Metal-forming tools, Seaming rolls, Ceramic Punches, Drawing dies

Processing methods

Dry Press, Precision Machining Processing