Description

Zirconia ceramics materials provide excellent erosion, corrosion and abrasion resistance along with temperature resistance, fracture toughness and strength. These ceramic components are used in extreme service applications that take advantage of their superior wear and corrosion resistance.

This material data has been provided by Innovacera.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

6 g/cm³

Show Supplier Material materials with Density of 6 g/cm³

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

2100 MPa

Show Supplier Material materials with Compressive strength of 2100 MPa

Elastic modulus

23.0 °C

210 GPa

Show Supplier Material materials with Elastic modulus of 210 GPa

Flexural strength

23.0 °C

1200 MPa

Show Supplier Material materials with Flexural strength of 1200 MPa

Hardness, Vickers

23.0 °C

1295 [-]

Show Supplier Material materials with Hardness, Vickers of 1295 [-]

Plane-Strain Fracture Toughnes

23.0 °C

6 - 7 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6 - 7 MPa·√m

Poisson's ratio

23.0 °C

0.22 - 0.23 [-]

Show Supplier Material materials with Poisson's ratio of 0.22 - 0.23 [-]

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1E-5 1/K

Specific heat capacity

23.0 °C

460 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

23.0 °C

2.5 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 2.5 W/(m·K)

Technological properties

Property
Application areas

Ceramic Valve components, Ceramic Pump liners, Ceramic Roller, Ceramic Plugs, Ceramic Sleeves, Ceramic Pistons, Ceramic Nozzle, Ceramic balls, Ceramic Spools, Ceramic Shaft, Ceramic Press tooling

Processing methods

Ceramic Injection Molding, Low Pressure Injection Molding, Cold Isostatic Press, Dry Press, Precision Machining Processing