Alumina Porous Ceramic

Want to keep this datasheet? Save it now in your required format

Description

Alumina porous ceramic filters are made from 80% aluminum oxide . The strong, uniform porous ceramic has 40-50% open porosity with a tortuous pore structure and is available in pore sizes ranging from 1 to 100 microns.

This material data has been provided by Innovacera.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.2 g/cm³

Show Supplier Material materials with Density of 2.2 g/cm³

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

600 MPa

Show Supplier Material materials with Compressive strength of 600 MPa

Flexural strength

23.0 °C

40 MPa

Show Supplier Material materials with Flexural strength of 40 MPa

Hardness, Rockwell A

23.0 °C

50 [-]

Show Supplier Material materials with Hardness, Rockwell A of 50 [-]

Technological properties

Property
Application areas

Filters for gases and liquids; Capillary Electrophoresis; Filtration for heavy metal ions (Cr, Ni etc) in water; High temperature chemical support for gas absorption; High efficiency flow through catalytic supports; Gas burners; Chromatography; Micro trapping systems and bio-catalytic supports; Vacuum holding plates (vacuum chunk); Nano-membrane supports for sensor applications; Micro-bubble diffusers; Fine or micro channels for electrophoresis; Chemical or bio reactor.

Processing methods

Low Pressure Injection Molding, Cold Isostatic Press, Dry Press, Precision Machining Processing