99.7%Boron Nitride

Want to keep this datasheet? Save it now in your required format

Description

Hexagonal Boron Nitride has a microstructure similar to that of Graphite. In both materials this structure, made up of layers of tiny platelets, is responsible for excellent machinability and low-friction properties. we called hexagonal boron nitride (HBN) or white graphite.

This material data has been provided by Innovacera.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.6 g/cm³

Show Supplier Material materials with Density of 1.6 g/cm³

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

45 MPa

Show Supplier Material materials with Compressive strength of 45 MPa

Flexural strength

23.0 °C

18 MPa

Show Supplier Material materials with Flexural strength of 18 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.5E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.5E-6 1/K

Thermal conductivity

23.0 °C

35 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 35 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

1.00E+16 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.00E+16 Ω·m

Technological properties

Property
Application areas

Thermal Management: very useful as a heat sink in high power electronic applications and electronic packaging materials. High Temperature Environments: equipment for plasma arc welding, diffusion source wafers, and semiconductor crystal growth equipment & processing. Molten Metal Handling: ideal for interface materials used in various molten metal processes.

Processing methods

Hot Pressed Sintering, Chemical Vapor Deposition