KHP®102 R360 - CuNiSi

Want to keep this datasheet? Save it now in your required format

Description

KHP®102 is a CuNiSi (Corson type) alloy. KHP®102 provides an outstanding combination of high electrical conductivity and good strength.

Equivalent Materials

This material data has been provided by Gebr. Kemper GmbH + Co. KG.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.9 g/cm³

Show Supplier Material materials with Density of 8.9 g/cm³

Mechanical

PropertyTemperatureValueComment

Bendability 180°, bw

23.0 °C

0 [-]

Show Supplier Material materials with Bendability 180°, bw of 0 [-]

Bendability 180°, gw

23.0 °C

0 [-]

Show Supplier Material materials with Bendability 180°, gw of 0 [-]

Bendability 90°, bw

23.0 °C

0 [-]

Show Supplier Material materials with Bendability 90°, bw of 0 [-]

Bendability 90°, gw

23.0 °C

0 [-]

Show Supplier Material materials with Bendability 90°, gw of 0 [-]

Elastic modulus

23.0 °C

127 GPa

Show Supplier Material materials with Elastic modulus of 127 GPa

Elongation A50

23.0 °C

12 %

Show Supplier Material materials with Elongation A50 of 12 %

min.

Tensile strength

23.0 °C

360 - 430 MPa

Show Supplier Material materials with Tensile strength of 360 - 430 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.68E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.68E-5 1/K

Thermal conductivity

23.0 °C

260 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 260 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

3.50E+7 S/m

Show Supplier Material materials with Electrical conductivity of 3.50E+7 S/m

Specific Electrical conductivity

60 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 60 % IACS

Chemical properties

PropertyValue

Copper

balance

Nickel

0.8 - 1.8 %

Show Supplier Material materials with Nickel of 0.8 - 1.8 %

Phosphorus

0.01 - 0.05 %

Show Supplier Material materials with Phosphorus of 0.01 - 0.05 %

Silicon

0.15 - 0.35 %

Show Supplier Material materials with Silicon of 0.15 - 0.35 %