KHP®109 R440 - CuNi1Sn0.9

Want to keep this datasheet? Save it now in your required format

Description

KHP®109 is a CuNiSn alloy. KHP®109 provides an excellent combination of high electrical conductivity and good strength.

Equivalent Materials

This material data has been provided by Gebr. Kemper GmbH + Co. KG.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.9 g/cm³

Show Supplier Material materials with Density of 8.9 g/cm³

Mechanical

PropertyTemperatureValueComment

Bendability 180°, bw

23.0 °C

1 [-]

Show Supplier Material materials with Bendability 180°, bw of 1 [-]

Bendability 180°, gw

23.0 °C

0 [-]

Show Supplier Material materials with Bendability 180°, gw of 0 [-]

Bendability 90°, bw

23.0 °C

1 [-]

Show Supplier Material materials with Bendability 90°, bw of 1 [-]

Bendability 90°, gw

23.0 °C

0 [-]

Show Supplier Material materials with Bendability 90°, gw of 0 [-]

Elastic modulus

23.0 °C

130 GPa

Show Supplier Material materials with Elastic modulus of 130 GPa

Elongation A50

23.0 °C

9 %

Show Supplier Material materials with Elongation A50 of 9 %

min.

Tensile strength

23.0 °C

440 - 520 MPa

Show Supplier Material materials with Tensile strength of 440 - 520 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.7E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.7E-5 1/K

Thermal conductivity

23.0 °C

161 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 161 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

2.30E+7 S/m

Show Supplier Material materials with Electrical conductivity of 2.30E+7 S/m

Specific Electrical conductivity

40 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 40 % IACS

Chemical properties

PropertyValue

Copper

balance

Nickel

0.8 - 1.2 %

Show Supplier Material materials with Nickel of 0.8 - 1.2 %

Phosphorus

0.03 - 0.07 %

Show Supplier Material materials with Phosphorus of 0.03 - 0.07 %

Tin

0.07 - 1.1 %

Show Supplier Material materials with Tin of 0.07 - 1.1 %