Description

Very high mechanical properties, very good resistance to sea-water corrosion and to oxidation, good impact and fatigue resistance, no sparks on impact, strictly amagnetic.

Related Standards

Equivalent Materials

This material data has been provided by Lebronze Alloys.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

8.6 g/cm³

Show Supplier Material materials with Density of 8.6 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperature

Elastic modulus

145 GPa

Show Supplier Material materials with Elastic modulus of 145 GPa at 23.0 °C

23.0 °C

Elongation

7 - 10 %

Show Supplier Material materials with Elongation of 7 - 10 % at 23.0 °C

23.0 °C

Hardness, Brinell

200 [-]

Show Supplier Material materials with Hardness, Brinell of 200 [-] at 23.0 °C

23.0 °C

Hardness, Rockwell C

15 [-]

Show Supplier Material materials with Hardness, Rockwell C of 15 [-] at 23.0 °C

23.0 °C

Hardness, Vickers

199 [-]

Show Supplier Material materials with Hardness, Vickers of 199 [-] at 23.0 °C

23.0 °C

Tensile strength

720 - 780 MPa

Show Supplier Material materials with Tensile strength of 720 - 780 MPa at 23.0 °C

23.0 °C

Yield strength

500 - 590 MPa

Show Supplier Material materials with Yield strength of 500 - 590 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

1.7E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.7E-5 1/K at 23.0 °C

23.0 °C

for 20-200°C

Thermal conductivity

30 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 30 W/(m·K) at 23.0 °C

23.0 °C

for 20-200°C

Electrical

PropertyValueTemperature

Electrical conductivity

5.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 5.00E+6 S/m at 23.0 °C

23.0 °C

Magnetic

PropertyValueTemperatureComment

Relative magnetic permeability

1.01 [-]

Show Supplier Material materials with Relative magnetic permeability of 1.01 [-] at 23.0 °C

23.0 °C

max

Technological properties

Property
Application areas

Summary of typical applications: Parts for marine industry, aerospace industry and electrical industry

Corrosion properties

Corrosion resistance rating: 5 out of 5

Friction

Friction behavior rating: 3 out of 5

General machinability

Machinability: 30 %