General Barium Dense Flint Glass

Want to keep this datasheet? Save it now in your required format

Description

Flint glasses are optical glasses with a relatively high refractive index in combination with a low Abbe number and, therfore, a high dispersion.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

3.1 - 3.6 g/cm³

Show Material materials with Density of 3.1 - 3.6 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

80 - 110 GPa

Show Material materials with Elastic modulus of 80 - 110 GPa

Hardness, Knoop, HK2

20.0 °C

500 - 650 [-]

Show Material materials with Hardness, Knoop, HK2 of 500 - 650 [-]

Poisson's ratio

20.0 °C

0.25 - 0.27 [-]

Show Material materials with Poisson's ratio of 0.25 - 0.27 [-]

Shear modulus

20.0 °C

34 - 39 GPa

Show Material materials with Shear modulus of 34 - 39 GPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

300.0 °C

8.1E-6 - 1.02E-5 1/K

Show Material materials with Coefficient of thermal expansion of 8.1E-6 - 1.02E-5 1/K

from 100 to 300°C

Glass transition temperature

500 - 620 °C

Show Material materials with Glass transition temperature of 500 - 620 °C

Specific heat capacity

20.0 °C

0.58 - 0.66 J/(kg·K)

Show Material materials with Specific heat capacity of 0.58 - 0.66 J/(kg·K)

Thermal conductivity

20.0 °C

0.26 - 1.06 W/(m·K)

Show Material materials with Thermal conductivity of 0.26 - 1.06 W/(m·K)

Optical

PropertyValue

Abbe number

35.87 - 42.5 [-]

Show Material materials with Abbe number of 35.87 - 42.5 [-]

Refractive index

1.6 - 1.72 [-]

Show Material materials with Refractive index of 1.6 - 1.72 [-]