Description

Zylon® PBO HS (high modulus) is a super fiber that features one of the highest levels of strength and modulus of elasticity (resistance to deformation) with flame & heat resistance. Tee HM fiber differsn from the AS fiber with a higher modulus and lower elongation at break.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

1.56 g/cm³

Show Material materials with Density of 1.56 g/cm³

Limiting oxygen index

20.0 °C

68 %

Show Material materials with Limiting oxygen index of 68 %

Water content

20.0 °C

0.6 %

Show Material materials with Water content of 0.6 %

Mechanical

PropertyTemperatureValue

Compressive strength

20.0 °C

561 MPa

Show Material materials with Compressive strength of 561 MPa

Elastic modulus

20.0 °C

270 GPa

Show Material materials with Elastic modulus of 270 GPa

Elongation

20.0 °C

2.5 %

Show Material materials with Elongation of 2.5 %

Tensile strength

20.0 °C

5800 MPa

Show Material materials with Tensile strength of 5800 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

20.0 °C

-6E-6 1/K

Show Material materials with Coefficient of thermal expansion of -6E-6 1/K

Melting point

650 °C

Show Material materials with Melting point of 650 °C

Electrical

PropertyTemperatureValueComment

Dielectric constant

20.0 °C

3 [-]

Show Material materials with Dielectric constant of 3 [-]

100kHz

Dissipation factor

20.0 °C

1E-3 [-]

Show Material materials with Dissipation factor of 1E-3 [-]

Technological properties

Property
Application areas

Protective cloth: Firefighter garmants, Safety gloves, Heat resistant garments. Sports: Bicycle Spokes, Bicycle tires, Yacht ropes, Tennis Racket, Badminton racket, Snowboard, Rider suits, Racing Car, Bow Strings. Industrial materials: Heat resistant felt, Cable cover for welding machine, Reinforcement for cements. Other: Speaker cone