SABIC® SUPEER™ 7318BE

Want to keep this datasheet? Save it now in your required format

Description

SABIC® SUPEER™ 7318BE is a metallocene ethylene-hexene copolymer. It has a good processability and performs well in a wide range of general purpose and high performance cast film applications. Films produced with this grade offer good impact strength, puncture resistance, sealing and optical properties. SABIC® SUPEER™ 7318BE is typically used for stretch and lamination films. Processing temperatures 210- 260 °C. Properties have been measured on cast film of 25 µm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

137.2 kN/m

Show Material materials with Tear strength of 137.2 kN/m

ASTM D1922

Tear strength, transverse

23.0 °C

166.6 kN/m

Show Material materials with Tear strength, transverse of 166.6 kN/m

ASTM D1922

Optical

PropertyValueComment

Haze

4 %

Show Material materials with Haze of 4 %

ASTM D1003

Technological properties

Property
Application areas

Stretch and lamination films.