LEXAN™ FR Resins ML5411H

Want to keep this datasheet? Save it now in your required format

Description

LEXAN ML5411H Polycarbonate (PC) is an injection moldable grade that is 9% glass fiber filled. It has a UL94 V2@1.47mm rating.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Impact strength, Charpy notched

-30.0 °C

9 kJ/m²

Show Material materials with Impact strength, Charpy notched of 9 kJ/m²

ISO 179/1eA

23.0 °C

10 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-30.0 °C

8 kJ/m²

Show Material materials with Impact strength, Izod notched of 8 kJ/m²

ISO 180/1A

23.0 °C

10 kJ/m²

Show Material materials with Impact strength, Izod notched of 10 kJ/m²

ISO 180/1A

Unlock all property charts

Impact strength, Izod unnotched

-30.0 °C

130 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 130 kJ/m²

ISO 180/1U

Impact strength, Charpy unnotched

No Break @ 23,-30°C | ISO 179/1eU

Technological properties

Property
Application areas

Electronic Components,Pump

Fillers

9% Glass Fiber

Processing methods

Drying Temperature: 120°C, Drying Time: 4-6hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 300-330°C, Nozzle Temperature: 280-320°C, Front - Zone 3 Temperature: 300-340°C, Middle - Zone 2 Temperature: 280-320°C, Rear - Zone 1 Temperature: 240-280°C, Hopper Temperature: 60-80°C, Mold Temperature: 80-100°C