Crastin® FG6134 NC010

Want to keep this datasheet? Save it now in your required format

Description

Crastin® FG6134 NC010 is an unreinforced, medium viscosity polybutylene terephthalate resin forinjection molding. It has been developed for consideration into applications such as parts for the food industry.FOOD CONTACTThis product is manufactured according to Good Manufacturing Practice (GMP) principles and generally accepted in food contact applications in Europe and the USA when meeting applicable use conditions. For details, individual compliance statements are available from your DuPont representative.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.3 g/cm³

Show Material materials with Density of 1.3 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.6 GPa

Show Material materials with Elastic modulus of 2.6 GPa

ISO 527-1/-2

Elongation

23.0 °C

90 %

Show Material materials with Elongation of 90 %

ISO 527-1/-2 | 50mm/min

Elongation at yield

23.0 °C

4 %

Show Material materials with Elongation at yield of 4 %

ISO 527-1/-2

Flexural strength

23.0 °C

85 MPa

Show Material materials with Flexural strength of 85 MPa

ISO 178

Impact strength, Charpy notched

23.0 °C

4 kJ/m²

Show Material materials with Impact strength, Charpy notched of 4 kJ/m²

ISO 179/1eA

Impact strength, Izod unnotched

23.0 °C

3.5 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 3.5 kJ/m²

ISO 180/1A

Poisson's ratio

23.0 °C

0.38 [-]

Show Material materials with Poisson's ratio of 0.38 [-]

Yield strength

23.0 °C

59 MPa

Show Material materials with Yield strength of 59 MPa

ISO 527-1/-2

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

180 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 180 °C

ISO 75-1/-2 | annealed

Heat deflection temperature, 1.80 MPa

60 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 60 °C

ISO 75-1/-2 | annealed

Melting point

225 °C

Show Material materials with Melting point of 225 °C

ISO 11357-1/-3 | 18°F/min

Flammability

Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, Oxygen index: 22 %, FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

32 g/10min

Show Material materials with Melt mass-flow rate of 32 g/10min

ISO 1133 | 250°C/2.16kg

Shrinkage

23.0 °C

1.6 %

Show Material materials with Shrinkage of 1.6 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

1.6 %

Show Material materials with Shrinkage, transverse of 1.6 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 120°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.04%, Melt Temperature Optimum: 250°C, Min. melt temperature: 240°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 80°C, Min. mold temperature: 30°C, Max. mold temperature: 130°C, Hold pressure range: ≥60MPa, Hold pressure time: 4s/mm, Back pressure: As low as possible, Ejection temperature: 170°C