Alloy 36 (Invar®) Controlled Expansion Alloy

View suppliers (21)
Want to keep this datasheet? Save it now in your required format

Description

1.3912 (FeNi36) is a 36% nickel-iron alloy. It exhibits a near zero rate of thermal expansion from around –100°C up to 200°C. This is around a tenth of the expansion rate of carbon steels. Alloy 36 also demonstrates a high retention of strength and toughness at cryogenic temperatures, making it suitable for a variety of low temperature or low expansion applications. The alloy is ideally suited to areas where dimensional changes due to temperature must be minimal, such as tooling for aerospace composites, radio and electronic devices and structural members in precision equipment such as lasers, measuring devices, thermostats and cryogenic instrumentation. Alloy 36 can also be utilised in combination with a high expansion material to crate mechanical movement with temperature in thermomechanical controls and switchgear.

Related Standards

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.13 g/cm³

Show Material materials with Density of 8.13 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

140 GPa

Show Material materials with Elastic modulus of 140 GPa

Elongation

23.0 °C

30 %

Show Material materials with Elongation of 30 %

Hardness, Vickers

23.0 °C

140 [-]

Show Material materials with Hardness, Vickers of 140 [-]

Tensile strength

23.0 °C

480 MPa

Show Material materials with Tensile strength of 480 MPa

Yield strength

23.0 °C

310 MPa

Show Material materials with Yield strength of 310 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

30.0 °C

1.2E-6 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-6 1/K

150.0 °C

2.7E-6 1/K

Show Material materials with Coefficient of thermal expansion of 2.7E-6 1/K

Melting point

1450 °C

Show Material materials with Melting point of 1450 °C

Specific heat capacity

23.0 °C

510 J/(kg·K)

Show Material materials with Specific heat capacity of 510 J/(kg·K)

Thermal conductivity

23.0 °C

10.5 W/(m·K)

Show Material materials with Thermal conductivity of 10.5 W/(m·K)

Chemical properties

PropertyValue

Iron

63 %

Show Material materials with Iron of 63 %

Manganese

0.6 %

Show Material materials with Manganese of 0.6 %

Nickel

36 %

Show Material materials with Nickel of 36 %

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

Technological properties

Property
Application areas

General: Positioning devices, bimetal thermostats, advanced composite moulds for aerospace industry, optical devices, echo boxes and filters for mobile telephones, magnetic shielding, small electrical transformers, metrology devices, scientific instruments, electrical circuit breakers, temperature regulators, clock balance wheels, pendulum clocks, precision condenser blades, radar and microwave cavity resonators, special electronic housings, seals, spacers, and specialized frames, high voltage transmission lines