Alloy 42 Controlled Expansion Alloy

View suppliers (15)
Want to keep this datasheet? Save it now in your required format

Description

1.3917 (FeNi42) is an iron-nickel alloy containing 42% nickel. It exhibits low thermal expansion characteristics over a range of temperatures, which makes it particularly suitable for use in glass and ceramic seals. It finds application in a variety of electronic components and lead frames. It shows the following features and properties:


  • Low coefficient of thermal expansion matched to silicon, ceramic materials such as alumina and beryllia and vitreous glass compounds
  • Low thermal expansion characteristics over a range of temperatures
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    8.15 g/cm³

    Show Material materials with Density of 8.15 g/cm³

    Mechanical

    PropertyTemperatureValue

    Elastic modulus

    23.0 °C

    145 GPa

    Show Material materials with Elastic modulus of 145 GPa

    Elongation

    23.0 °C

    30 %

    Show Material materials with Elongation of 30 %

    Hardness, Vickers

    23.0 °C

    140 [-]

    Show Material materials with Hardness, Vickers of 140 [-]

    Tensile strength

    23.0 °C

    500 MPa

    Show Material materials with Tensile strength of 500 MPa

    Yield strength

    23.0 °C

    300 MPa

    Show Material materials with Yield strength of 300 MPa

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    30.0 °C

    4E-6 1/K

    Show Material materials with Coefficient of thermal expansion of 4E-6 1/K

    450.0 °C

    7.4E-6 1/K

    Show Material materials with Coefficient of thermal expansion of 7.4E-6 1/K

    Melting point

    1425 °C

    Show Material materials with Melting point of 1425 °C

    Specific heat capacity

    23.0 °C

    500 J/(kg·K)

    Show Material materials with Specific heat capacity of 500 J/(kg·K)

    Thermal conductivity

    23.0 °C

    12.5 W/(m·K)

    Show Material materials with Thermal conductivity of 12.5 W/(m·K)

    Chemical properties

    PropertyValue

    Iron

    58 %

    Show Material materials with Iron of 58 %

    Manganese

    0.8 %

    Show Material materials with Manganese of 0.8 %

    Nickel

    41 %

    Show Material materials with Nickel of 41 %

    Technological properties

    Property
    Application areas

    It can be found as a sealing material in semiconductor packages, electronic tubes, CRT electron guns, microelectronic components, thermostat rods, vacuum devices and electric industrial lamps