Alloy K (Kovar®) Controlled Expansion Alloy

View suppliers (15)
Want to keep this datasheet? Save it now in your required format

Description

1.3981 (FeNi29Co17) is an iron-nickel-cobalt alloy whose chemical composition is controlled within narrow limits to ensure precise and uniform thermal expansion and mechanical characteristics. These properties make it an ideal alloy for use in high integrity glass-to-metal and ceramic-to-metal seals, particularly where the application requires resistance to thermal shock. It shows the following features and properties:


  • Uniform thermal expansion characteristics
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    8.25 g/cm³

    Show Material materials with Density of 8.25 g/cm³

    Mechanical

    PropertyTemperatureValue

    Elastic modulus

    23.0 °C

    139 GPa

    Show Material materials with Elastic modulus of 139 GPa

    Elongation

    23.0 °C

    30 %

    Show Material materials with Elongation of 30 %

    Hardness, Vickers

    23.0 °C

    160 [-]

    Show Material materials with Hardness, Vickers of 160 [-]

    Tensile strength

    23.0 °C

    540 MPa

    Show Material materials with Tensile strength of 540 MPa

    Yield strength

    23.0 °C

    380 MPa

    Show Material materials with Yield strength of 380 MPa

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    30.0 °C

    4.6E-6 1/K

    Show Material materials with Coefficient of thermal expansion of 4.6E-6 1/K

    450.0 °C

    5.5E-6 1/K

    Show Material materials with Coefficient of thermal expansion of 5.5E-6 1/K

    Melting point

    1450 °C

    Show Material materials with Melting point of 1450 °C

    Specific heat capacity

    23.0 °C

    500 J/(kg·K)

    Show Material materials with Specific heat capacity of 500 J/(kg·K)

    Thermal conductivity

    23.0 °C

    17 W/(m·K)

    Show Material materials with Thermal conductivity of 17 W/(m·K)

    Chemical properties

    PropertyValue

    Cobalt

    17 %

    Show Material materials with Cobalt of 17 %

    Iron

    53 %

    Show Material materials with Iron of 53 %

    Nickel

    29 %

    Show Material materials with Nickel of 29 %

    Technological properties

    Property
    Application areas

    General: Power and microwave tubes, transistors and diodes, lids and closures in a variety of hybrid electronic circuit packages.