C103 (Cu-OF) is a commercially pure grade of oxygen-free copper manufactured by pouring in a protective gas atmosphere or vacuum. The absence of oxygen ensures high levels of electrical conductivity and low susceptibility to embrittlement when heated in a reducing atmosphere.

Related Standards

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValueComment

Copper

99.95 %

Show Material materials with Copper of 99.95 %

min.

Technological properties

Property
Application areas

General: Radar and other electronic equipment, anodes for vacuum tubes, glass to metal seals in electronic equipment, thermostatic control valves, rotor conductors for large generators and motors, electrical equipment for service at elevated temperatures in the presence of reducing gases and anodes for electroplating, particularly in cyanide baths