Description

2.4856 (NiCr22Mo9Nb) is a nickel-chromium-molybdenum alloy with a small niobium and tantalum addition. It is an excellent general purpose material for elevated temperature use in high strength, oxidation problem areas and finds particular application in the aerospace and offshore oil & gas industries. It shows excellent resistance to a variety of corrosive media. It shows the following features and properties:


  • Strength retained up to 450ºC
  • Very good resistance to corrosion fatigue
  • High pitting, crevice and stress corrosion resistance
  • Excellent oxidation resistance
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    8.44 g/cm³

    Show Material materials with Density of 8.44 g/cm³

    Mechanical

    PropertyTemperatureValue

    Elastic modulus

    23.0 °C

    207 GPa

    Show Material materials with Elastic modulus of 207 GPa

    Elongation

    23.0 °C

    30 %

    Show Material materials with Elongation of 30 %

    Tensile strength

    23.0 °C

    690 - 830 MPa

    Show Material materials with Tensile strength of 690 - 830 MPa

    Yield strength Rp0.2

    23.0 °C

    275 - 415 MPa

    Show Material materials with Yield strength Rp0.2 of 275 - 415 MPa

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    1.28E-5 1/K

    Show Material materials with Coefficient of thermal expansion of 1.28E-5 1/K

    for 0-100°C

    Melting point

    1290 - 1350 °C

    Show Material materials with Melting point of 1290 - 1350 °C

    Thermal conductivity

    23.0 °C

    9.8 W/(m·K)

    Show Material materials with Thermal conductivity of 9.8 W/(m·K)

    Electrical

    PropertyTemperatureValue

    Electrical resistivity

    23.0 °C

    1.32E-6 Ω·m

    Show Material materials with Electrical resistivity of 1.32E-6 Ω·m

    Magnetic

    PropertyTemperatureValueComment

    Relative magnetic permeability

    23.0 °C

    1 [-]

    Show Material materials with Relative magnetic permeability of 1 [-]

    max.

    Chemical properties

    PropertyValueComment

    Aluminium

    0.2 %

    Show Material materials with Aluminium of 0.2 %

    Chromium

    22 %

    Show Material materials with Chromium of 22 %

    Iron

    2 %

    Show Material materials with Iron of 2 %

    Molybdenum

    9 %

    Show Material materials with Molybdenum of 9 %

    Nickel

    58 - 61 %

    Show Material materials with Nickel of 58 - 61 %

    Niobium

    3.5 %

    Show Material materials with Niobium of 3.5 %

    Nb+Ta

    Tantalum

    3.5 %

    Show Material materials with Tantalum of 3.5 %

    Nb+Ta

    Titanium

    0.2 %

    Show Material materials with Titanium of 0.2 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Components where exposure to sea water and high mechanical stresses are required, oil and gas production where hydrogen sulphide and elementary sulphur exist at temperature in excess of 150C, flare stacks, hydrocarbon processing from tar-sand and oil-shale recovery projects;Chemical processing: Flue gas desulphurisation plant, flare stacks, offshore sour oil and gas production, waste incineration, phosphoric acid production and nuclear fuel processing

    Corrosion properties

    Very good corrosion resistance