Description

2.4819 (NiMo16Cr15W) is a wrought nickel-chromium-molybdenum-tungsten alloy which displays remarkable corrosion resistance in a very wide range of processing environments. It offers excellent resistance to stress corrosion cracking and oxidising atmospheres up to 1040°C, whilst the high molybdenum content gives the alloy its excellent resistance to pitting and crevice corrosion. The low carbon content prevents the formation of grain boundary precipitates during welding. It shows the following features and properties:


  • Excellent resistance to pitting and corrosion
  • High mechanical properties
  • Excellent resistance to oxidising atmospheres up to 1040°C
  • Very high resistance to many aggressive chemicals
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Mechanical

    PropertyTemperatureValue

    Elongation

    23.0 °C

    40 %

    Show Material materials with Elongation of 40 %

    Tensile strength

    23.0 °C

    690 MPa

    Show Material materials with Tensile strength of 690 MPa

    Yield strength Rp0.2

    23.0 °C

    283 MPa

    Show Material materials with Yield strength Rp0.2 of 283 MPa

    Chemical properties

    PropertyValue

    Chromium

    15.5 %

    Show Material materials with Chromium of 15.5 %

    Iron

    5.5 %

    Show Material materials with Iron of 5.5 %

    Molybdenum

    16 %

    Show Material materials with Molybdenum of 16 %

    Nickel

    57 %

    Show Material materials with Nickel of 57 %

    Tungsten

    3.8 %

    Show Material materials with Tungsten of 3.8 %

    Technological properties

    Property
    Application areas

    Chemical processing: Arduous areas of flue gas desulphurisation plants, critical components in sewage treatment, chemical and petrochemical plants, waste incineration, sour gas production and organic acid processing

    Corrosion properties

    Excellent corrosion resistance