Monel Alloy 400 Nickel Alloy

View suppliers (61)
Want to keep this datasheet? Save it now in your required format

Description

2.4360 (NiCu30Fe) is a nickel-copper alloy resistant to seawater and steam at high temperatures and widely used in the chemical, oil and marine industries. As a solution strengthened material, Monel Alloy 400 displays good strength, toughness and corrosion resistance at temperatures up to 400°C. It is supplied by Columbia Metals in the cold worked condition as standard. It shows the following features and properties:


  • Good strength and toughness
  • Excellent corrosion resistance in marine environments
  • Good resistance to non oxidising acids, alkalis and salts
  • Not susceptible to chloride stress corrosion cracking
  • Readily weldable
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    8.8 g/cm³

    Show Material materials with Density of 8.8 g/cm³

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    180 GPa

    Show Material materials with Elastic modulus of 180 GPa

    Elongation

    23.0 °C

    20 - 35 %

    Show Material materials with Elongation of 20 - 35 %

    Hardness, Rockwell C

    23.0 °C

    35 [-]

    Show Material materials with Hardness, Rockwell C of 35 [-]

    max.

    Tensile strength

    23.0 °C

    480 - 600 MPa

    Show Material materials with Tensile strength of 480 - 600 MPa

    Yield strength Rp0.2

    23.0 °C

    170 - 415 MPa

    Show Material materials with Yield strength Rp0.2 of 170 - 415 MPa

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    23.0 °C

    1.39E-5 1/K

    Show Material materials with Coefficient of thermal expansion of 1.39E-5 1/K

    Melting point

    1300 - 1350 °C

    Show Material materials with Melting point of 1300 - 1350 °C

    Thermal conductivity

    23.0 °C

    22 W/(m·K)

    Show Material materials with Thermal conductivity of 22 W/(m·K)

    Electrical

    PropertyValue

    Specific Electrical conductivity

    34 % IACS

    Show Material materials with Specific Electrical conductivity of 34 % IACS

    Chemical properties

    PropertyValueComment

    Copper

    28 - 34 %

    Show Material materials with Copper of 28 - 34 %

    Iron

    2.5 %

    Show Material materials with Iron of 2.5 %

    max.

    Manganese

    2 %

    Show Material materials with Manganese of 2 %

    Nickel

    63 %

    Show Material materials with Nickel of 63 %

    min., (Ni+Co)

    Technological properties

    Property
    Application areas

    Offshore & marine: Marine components, shafts, splash zone sheathing and fasteners;Chemical processing: Components for the manufacture of chlorinated solvents, salt production, ethyl chloride purification and numerous other areas of process plant;Other: Wire netting for insulation, oil well recovery pumps and crude oil distillation towers

    Cold Forming

    It can be cold worked

    Corrosion properties

    Excellent corrosion resistance in marine environments

    General machinability

    It is readily machinable

    Hot forming

    It can be hot worked