EFI Alloy 79 Annealed Strip/Coil

Alternative and trade names
Magnifer 7904®, HyMu 80®, Hipernom®, Moly-Permalloy, Permalloy 80
Want to keep this datasheet? Save it now in your required format

Description

A soft magnetic alloy consisting of 80% nickel, 5% molybdenum, and balance iron used where extremely high initial & maximum permeability and minimum hysteresis is needed.

Related Standards

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.74 g/cm³

Show Material materials with Density of 8.74 g/cm³

Dimension

PropertyValueComment

Length

3048 mm

Show Material materials with Length of 3048 mm

Mill random length

Thickness

0.1 - 0.64 mm

Show Material materials with Thickness of 0.1 - 0.64 mm

Width

304.8 mm

Show Material materials with Width of 304.8 mm

Dimensions

Available thicknesses: 0.10mm, 0.25mm, 0.36mm, 0.51mm, 0.64mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

217 GPa

Show Material materials with Elastic modulus of 217 GPa

Elongation

23.0 °C

40 %

Show Material materials with Elongation of 40 %

in 2 in.

Hardness, Rockwell B

23.0 °C

85 [-]

Show Material materials with Hardness, Rockwell B of 85 [-]

Tensile strength

23.0 °C

676 MPa

Show Material materials with Tensile strength of 676 MPa

Yield strength

23.0 °C

262 MPa

Show Material materials with Yield strength of 262 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

450.0 °C

1.36E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.36E-5 1/K

from 20°C to the mentioned temperature

Melting point

1454 °C

Show Material materials with Melting point of 1454 °C

Specific heat capacity

23.0 °C

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

23.0 °C

35 W/(m·K)

Show Material materials with Thermal conductivity of 35 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

5.9E-7 Ω·m

Show Material materials with Electrical resistivity of 5.9E-7 Ω·m

Magnetic

PropertyTemperatureValue

Coercive force

23.0 °C

1.19 A/m

Show Material materials with Coercive force of 1.19 A/m

Curie temperature

460 °C

Show Material materials with Curie temperature of 460 °C

Relative magnetic permeability

23.0 °C

230000 [-]

Show Material materials with Relative magnetic permeability of 230000 [-]

Saturation induction

23.0 °C

0.8 T

Show Material materials with Saturation induction of 0.8 T

Chemical properties

PropertyValue

Carbon

0.03 %

Show Material materials with Carbon of 0.03 %

Iron

Balance

Manganese

0.95 %

Show Material materials with Manganese of 0.95 %

Molybdenum

5 %

Show Material materials with Molybdenum of 5 %

Nickel

80 %

Show Material materials with Nickel of 80 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.42 %

Show Material materials with Silicon of 0.42 %

Sulfur

8E-3 %

Show Material materials with Sulfur of 8E-3 %

Technological properties

Property
Application areas

Common applications of EFI ALLOY 79 are: Toroidal tape-wound cores - instrument transformers, inductive components, earth-leakage circuit breakers; Magnetic shielding - shielding cans, shielding films, spatial shielding arrangements; Ground fault circuit interrupters; Electromagnetic relay parts; Laminations - transformer laminations, transformer cores for modems, stampled rings for electronic earth-leakage breakers, operating at a low magnetic field strengths