Description

A controlled expansion nickel iron alloy, consisting of nearly 41% nickel, balance iron.

Related Standards

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.12 g/cm³

Show Material materials with Density of 8.12 g/cm³

Dimension

PropertyValue

Length

1828 mm

Show Material materials with Length of 1828 mm

Thickness

4.8 - 7.1 mm

Show Material materials with Thickness of 4.8 - 7.1 mm

Width

381 mm

Show Material materials with Width of 381 mm

Dimensions

Available thicknesses: 4.8mm, 7.1mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

148 GPa

Show Material materials with Elastic modulus of 148 GPa

Elongation

23.0 °C

30 %

Show Material materials with Elongation of 30 %

in 2 in.

Hardness, Rockwell B

23.0 °C

80 [-]

Show Material materials with Hardness, Rockwell B of 80 [-]

Tensile strength

23.0 °C

566 MPa

Show Material materials with Tensile strength of 566 MPa

Yield strength

23.0 °C

235 MPa

Show Material materials with Yield strength of 235 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

4.2E-6 1/K

Show Material materials with Coefficient of thermal expansion of 4.2E-6 1/K

from 30°C to the mentioned temperature

150.0 °C

4.2E-6 1/K

Show Material materials with Coefficient of thermal expansion of 4.2E-6 1/K

from 30°C to the mentioned temperature

200.0 °C

4.2E-6 1/K

Show Material materials with Coefficient of thermal expansion of 4.2E-6 1/K

from 30°C to the mentioned temperature

250.0 °C

4.2E-6 1/K

Show Material materials with Coefficient of thermal expansion of 4.2E-6 1/K

from 30°C to the mentioned temperature

300.0 °C

4E-6 - 4.7E-6 1/K

Show Material materials with Coefficient of thermal expansion of 4E-6 - 4.7E-6 1/K

from 30°C to the mentioned temperature

325.0 °C

4.6E-6 1/K

Show Material materials with Coefficient of thermal expansion of 4.6E-6 1/K

from 30°C to the mentioned temperature

350.0 °C

5E-6 1/K

Show Material materials with Coefficient of thermal expansion of 5E-6 1/K

from 30°C to the mentioned temperature

375.0 °C

5.6E-6 1/K

Show Material materials with Coefficient of thermal expansion of 5.6E-6 1/K

from 30°C to the mentioned temperature

400.0 °C

6.1E-6 1/K

Show Material materials with Coefficient of thermal expansion of 6.1E-6 1/K

from 30°C to the mentioned temperature

425.0 °C

6.7E-6 1/K

Show Material materials with Coefficient of thermal expansion of 6.7E-6 1/K

from 30°C to the mentioned temperature

450.0 °C

6.7E-6 - 7.4E-6 1/K

Show Material materials with Coefficient of thermal expansion of 6.7E-6 - 7.4E-6 1/K

from 30°C to the mentioned temperature

475.0 °C

7.7E-6 1/K

Show Material materials with Coefficient of thermal expansion of 7.7E-6 1/K

from 30°C to the mentioned temperature

500.0 °C

8.1E-6 1/K

Show Material materials with Coefficient of thermal expansion of 8.1E-6 1/K

from 30°C to the mentioned temperature

525.0 °C

8.5E-6 1/K

Show Material materials with Coefficient of thermal expansion of 8.5E-6 1/K

from 30°C to the mentioned temperature

550.0 °C

8.9E-6 1/K

Show Material materials with Coefficient of thermal expansion of 8.9E-6 1/K

from 30°C to the mentioned temperature

600.0 °C

9.6E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.6E-6 1/K

from 30°C to the mentioned temperature

700.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

from 30°C to the mentioned temperature

800.0 °C

1.14E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.14E-5 1/K

from 30°C to the mentioned temperature

900.0 °C

1.23E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.23E-5 1/K

from 30°C to the mentioned temperature

1004.0 °C

1.32E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K

from 30°C to the mentioned temperature

Melting point

1427 °C

Show Material materials with Melting point of 1427 °C

Specific heat capacity

23.0 °C

502 J/(kg·K)

Show Material materials with Specific heat capacity of 502 J/(kg·K)

Thermal conductivity

23.0 °C

11 W/(m·K)

Show Material materials with Thermal conductivity of 11 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

6.8E-7 Ω·m

Show Material materials with Electrical resistivity of 6.8E-7 Ω·m

Magnetic

PropertyValue

Curie temperature

380 °C

Show Material materials with Curie temperature of 380 °C

Chemical properties

PropertyValue

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Chromium

0.03 %

Show Material materials with Chromium of 0.03 %

Iron

Balance

Nickel

41 %

Show Material materials with Nickel of 41 %

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %

Technological properties

Property
Application areas

Common applications of Alloy 42: Thermostats, thermoswitches, integrated circuit lead frames, Glass to metal seals for a wide variety of electronic tubes, hermetic packages, and automotive and industrial lamps., high temperature curing of aircraft thermoset composites