A controlled expansion alloy, consisting of 51% Nickel, balance Iron.

Related Standards

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.3 g/cm³

Show Material materials with Density of 8.3 g/cm³

Dimension

PropertyValue

Thickness

0.25 - 0.38 mm

Show Material materials with Thickness of 0.25 - 0.38 mm

Dimensions

Available thicknesses: 0.254mm, 0.381mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

159 GPa

Show Material materials with Elastic modulus of 159 GPa

Elongation

23.0 °C

35 %

Show Material materials with Elongation of 35 %

in 2 in.

Hardness, Rockwell B

23.0 °C

80 [-]

Show Material materials with Hardness, Rockwell B of 80 [-]

Tensile strength

23.0 °C

552 MPa

Show Material materials with Tensile strength of 552 MPa

Yield strength

23.0 °C

276 MPa

Show Material materials with Yield strength of 276 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

from 30°C to the mentioned temperature

150.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

from 30°C to the mentioned temperature

200.0 °C

1.04E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.04E-5 1/K

from 30°C to the mentioned temperature

250.0 °C

1.04E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.04E-5 1/K

from 30°C to the mentioned temperature

300.0 °C

1.02E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.02E-5 1/K

from 30°C to the mentioned temperature

350.0 °C

1.02E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.02E-5 1/K

from 30°C to the mentioned temperature

400.0 °C

1.01E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.01E-5 1/K

from 30°C to the mentioned temperature

450.0 °C

1.07E-5 - 9.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.07E-5 - 9.6E-5 1/K

from 30°C to the mentioned temperature

475.0 °C

1.01E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.01E-5 1/K

from 30°C to the mentioned temperature

500.0 °C

1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1E-5 1/K

from 30°C to the mentioned temperature

525.0 °C

1.04E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.04E-5 1/K

from 30°C to the mentioned temperature

550.0 °C

1.02E-5 - 1.07E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.02E-5 - 1.07E-5 1/K

from 30°C to the mentioned temperature

600.0 °C

1.08E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.08E-5 1/K

from 30°C to the mentioned temperature

700.0 °C

1.17E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.17E-5 1/K

from 30°C to the mentioned temperature

800.0 °C

1.25E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.25E-5 1/K

from 30°C to the mentioned temperature

900.0 °C

1.33E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.33E-5 1/K

from 30°C to the mentioned temperature

1011.0 °C

1.42E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.42E-5 1/K

from 30°C to the mentioned temperature

Melting point

1427 °C

Show Material materials with Melting point of 1427 °C

Specific heat capacity

23.0 °C

502 J/(kg·K)

Show Material materials with Specific heat capacity of 502 J/(kg·K)

Thermal conductivity

23.0 °C

14 W/(m·K)

Show Material materials with Thermal conductivity of 14 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

4.4E-7 Ω·m

Show Material materials with Electrical resistivity of 4.4E-7 Ω·m

Magnetic

PropertyValue

Curie temperature

530 °C

Show Material materials with Curie temperature of 530 °C

Chemical properties

PropertyValue

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Chromium

0.03 %

Show Material materials with Chromium of 0.03 %

Iron

Balance

Nickel

50.5 %

Show Material materials with Nickel of 50.5 %

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %

Technological properties

Property
Application areas

Common applications of Alloy 52: Pin feed-throughs for semiconductor devices, glass-to-metal sealing with soft glass for mercury switches and semiconductor devices

Looking for suppliers of this material? Click to see 5 supplier of Alloy 52 Strip/Coil on Matmatch