The material: 'Nickel 200 Bar' you were looking for has been superseded by the one below.

Nickel 200 Bar

Want to keep this datasheet? Save it now in your required format

Description

Commercially pure, unalloyed Nickel.

Related Standards

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.89 g/cm³

Show Material materials with Density of 8.89 g/cm³

Dimension

PropertyValue

Width

3.18 - 57.15 mm

Show Material materials with Width of 3.18 - 57.15 mm

Dimensions

Available widths: 3.2mm, 4.8mm, 6.4mm, 7.9mm, 9.5mm, 12.7mm, 15.9mm, 19.1mm, 22.2mm, 28.6mm, 31.8mm, 44.5mm, 50.8mm, 57.2mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

207 GPa

Show Material materials with Elastic modulus of 207 GPa

Elongation

23.0 °C

40 %

Show Material materials with Elongation of 40 %

in 2 in.

Hardness, Rockwell B

23.0 °C

80 [-]

Show Material materials with Hardness, Rockwell B of 80 [-]

Tensile strength

23.0 °C

449 MPa

Show Material materials with Tensile strength of 449 MPa

Yield strength

23.0 °C

138 MPa

Show Material materials with Yield strength of 138 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K

from 30°C to the mentioned temperature

Melting point

1440 °C

Show Material materials with Melting point of 1440 °C

Specific heat capacity

23.0 °C

452 J/(kg·K)

Show Material materials with Specific heat capacity of 452 J/(kg·K)

Thermal conductivity

23.0 °C

79 W/(m·K)

Show Material materials with Thermal conductivity of 79 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

8.5E-8 Ω·m

Show Material materials with Electrical resistivity of 8.5E-8 Ω·m

Magnetic

PropertyValue

Curie temperature

360 °C

Show Material materials with Curie temperature of 360 °C

Chemical properties

PropertyValue

Carbon

0.07 %

Show Material materials with Carbon of 0.07 %

Iron

0.25 %

Show Material materials with Iron of 0.25 %

Nickel

99.5 %

Show Material materials with Nickel of 99.5 %

Silicon

0.25 %

Show Material materials with Silicon of 0.25 %

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %

Technological properties

Property
Application areas

Common applications of Nickel 200: Getter tabs, heating element sheathing, anodes, fuel cells, special purpose electron tubes, transistor enclosures, cathode shields, spark gaps