General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.89 g/cm³ Show Material materials with Density of 8.89 g/cm³ |
Dimension
Property | Value |
---|---|
Width | 3.18 - 57.15 mm Show Material materials with Width of 3.18 - 57.15 mm |
Dimensions | Available widths: 3.2mm, 4.8mm, 6.4mm, 7.9mm, 9.5mm, 12.7mm, 15.9mm, 19.1mm, 22.2mm, 28.6mm, 31.8mm, 44.5mm, 50.8mm, 57.2mm |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 207 GPa Show Material materials with Elastic modulus of 207 GPa | |
Elongation | 23.0 °C | 40 % Show Material materials with Elongation of 40 % | in 2 in. |
Hardness, Rockwell B | 23.0 °C | 80 [-] Show Material materials with Hardness, Rockwell B of 80 [-] | |
Tensile strength | 23.0 °C | 449 MPa Show Material materials with Tensile strength of 449 MPa | |
Yield strength | 23.0 °C | 138 MPa Show Material materials with Yield strength of 138 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K | from 30°C to the mentioned temperature |
Melting point | 1440 °C Show Material materials with Melting point of 1440 °C | ||
Specific heat capacity | 23.0 °C | 452 J/(kg·K) Show Material materials with Specific heat capacity of 452 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 75 W/(m·K) Show Material materials with Thermal conductivity of 75 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 9.5E-8 Ω·m Show Material materials with Electrical resistivity of 9.5E-8 Ω·m |
Magnetic
Property | Value |
---|---|
Curie temperature | 360 °C Show Material materials with Curie temperature of 360 °C |
Chemical properties
Property | Value |
---|---|
Carbon | 0.07 % Show Material materials with Carbon of 0.07 % |
Iron | 0.2 % Show Material materials with Iron of 0.2 % |
Magnesium | 0.01 - 0.1 % Show Material materials with Magnesium of 0.01 - 0.1 % |
Nickel | 99.5 % Show Material materials with Nickel of 99.5 % |
Silicon | 0.15 % Show Material materials with Silicon of 0.15 % |
Sulfur | 8E-3 % Show Material materials with Sulfur of 8E-3 % |
Titanium | 0.05 % Show Material materials with Titanium of 0.05 % |
Technological properties
Property | ||
---|---|---|
Application areas | Common applications of Nickel 205: Getter tabs, heating element sheathing, anodes, fuel cells, special purpose electron tubes, transistor enclosures, cathode shields, spark gaps |