Description

Commercially pure, unalloyed Nickel.

Related Standards

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.89 g/cm³

Show Material materials with Density of 8.89 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

207 GPa

Show Material materials with Elastic modulus of 207 GPa

Elongation

23.0 °C

40 %

Show Material materials with Elongation of 40 %

in 2 in.

Hardness, Rockwell B

23.0 °C

80 [-]

Show Material materials with Hardness, Rockwell B of 80 [-]

Tensile strength

23.0 °C

449 MPa

Show Material materials with Tensile strength of 449 MPa

Yield strength

23.0 °C

138 MPa

Show Material materials with Yield strength of 138 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K

from 30°C to the mentioned temperature

Melting point

1440 °C

Show Material materials with Melting point of 1440 °C

Specific heat capacity

23.0 °C

452 J/(kg·K)

Show Material materials with Specific heat capacity of 452 J/(kg·K)

Thermal conductivity

23.0 °C

86 W/(m·K)

Show Material materials with Thermal conductivity of 86 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

7.5E-8 Ω·m

Show Material materials with Electrical resistivity of 7.5E-8 Ω·m

Magnetic

PropertyValue

Curie temperature

360 °C

Show Material materials with Curie temperature of 360 °C

Chemical properties

PropertyValue

Carbon

0.02 %

Show Material materials with Carbon of 0.02 %

Cobalt

1E-3 %

Show Material materials with Cobalt of 1E-3 %

Iron

5E-3 %

Show Material materials with Iron of 5E-3 %

Nickel

99.97 %

Show Material materials with Nickel of 99.97 %

Silicon

1E-3 %

Show Material materials with Silicon of 1E-3 %

Sulfur

1E-3 %

Show Material materials with Sulfur of 1E-3 %

Technological properties

Property
Application areas

Common applications of Nickel 270: Anode plates, hydrogen thyratron components, passive cathodes, cathodes shanks, plater bars, transistor enclosures