Lithium Foil 99.9% Purity (LI000260)

Want to keep this datasheet? Save it now in your required format

Description

Lithium is a soft, silver metal, and is the first member of the alkali group of metals. It is the lightest of all metals and, whilst resembling sodium chemically, it is less active. As is the case for other alkali group elements, it is obtained by the electrolysis of the fused halides.


The abundance of lithium in the earth's crust is 20 ppm. Lithium reacts slowly in water and in air where it eventually forms a black coating of oxide. This means that this metal tends to be stored under oil to prevent deterioration.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

0.53 g/cm³

Show Material materials with Density of 0.53 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

4.91 GPa

Show Material materials with Elastic modulus of 4.91 GPa

Hardness, Vickers

23.0 °C

5 [-]

Show Material materials with Hardness, Vickers of 5 [-]

Poisson's ratio

23.0 °C

0.36 [-]

Show Material materials with Poisson's ratio of 0.36 [-]

Thermal

PropertyTemperatureValue

Boiling point

1342 °C

Show Material materials with Boiling point of 1342 °C

Coefficient of thermal expansion

100.0 °C

5.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 5.6E-5 1/K

Latent heat of evaporation

19600 J/g

Show Material materials with Latent heat of evaporation of 19600 J/g

Latent heat of fusion

422 J/g

Show Material materials with Latent heat of fusion of 422 J/g

Melting point

180.5 °C

Show Material materials with Melting point of 180.5 °C

Specific heat capacity

23.0 °C

3560 J/(kg·K)

Show Material materials with Specific heat capacity of 3560 J/(kg·K)

Thermal conductivity

100.0 °C

84.8 W/(m·K)

Show Material materials with Thermal conductivity of 84.8 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

9.29E-8 Ω·m

Show Material materials with Electrical resistivity of 9.29E-8 Ω·m

Temperature coefficient of resistance

23.0 °C

4.35E-3 1/K

Show Material materials with Temperature coefficient of resistance of 4.35E-3 1/K

Thermal electromotive force

23.0 °C

1.82 mV

Show Material materials with Thermal electromotive force of 1.82 mV

cold 0°C - hot 100°C

Chemical properties

PropertyValue

Aluminium

5E-4 %

Show Material materials with Aluminium of 5E-4 %

Calcium

1E-3 %

Show Material materials with Calcium of 1E-3 %

Chlorine

4E-3 %

Show Material materials with Chlorine of 4E-3 %

Iron

5E-3 %

Show Material materials with Iron of 5E-3 %

Lithium

balance

Nitrogen

4E-3 %

Show Material materials with Nitrogen of 4E-3 %

Potassium

6E-3 %

Show Material materials with Potassium of 6E-3 %

Silicon

1E-3 %

Show Material materials with Silicon of 1E-3 %

Sodium

8E-3 %

Show Material materials with Sodium of 8E-3 %

Technological properties

Property
Application areas

Lithium and its compounds find applications in the manufacture of glass and ceramics.