Boron Nitride Nanotubes (90% purity)

Want to keep this datasheet? Save it now in your required format

Description

Boron Nitride Nanotube is a next-generation Nano-material which will lead the 4th industrial revolution. Boron nitride nanotubes (BNNTs) are another form of boron nitride.


Structurally they are nano-cylinders with sub-micrometre diameters and micrometre lengths. They are composed of hexagonal boron nitride, constructed by combining boron and nitrogen.


The key features that represent BNNTs are light weight, mechanical strength, thermal and chemical stability, high electrical resistivity and neutron absorption capacity.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Nanotube diameter

50 nm

Show Material materials with Nanotube diameter of 50 nm

Nanotube length

10 µm

Show Material materials with Nanotube length of 10 µm

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

1180 GPa

Show Material materials with Elastic modulus of 1180 GPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1E-6 1/K

Show Material materials with Coefficient of thermal expansion of 1E-6 1/K

Max service temperature

800 °C

Show Material materials with Max service temperature of 800 °C

in air

Thermal conductivity

23.0 °C

600 W/(m·K)

Show Material materials with Thermal conductivity of 600 W/(m·K)

experimental value

Electrical

PropertyValue

Band gap

5.5 eV

Show Material materials with Band gap of 5.5 eV

Technological properties

Property
Application areas

Electric insulation thermal conducting: Electrical insulation / Heat radiating sheet / Adhesive material, Highly bright LED packing materials, Piezoelectric sensors (energy harvesting), Ultra-small ultraviolet laser / Nano cable, Visible light emitter, etc; High temperature structural applications: Light and tough structural materials for space and artificial satellite, Super plasticity ceramic for high temperature, Aircraft / Reinforced ceramic material for spacecraft, Neutron detection sensor for high temperature; Biomedical Applications: BNCT drug target, Drug delivering agent for cancer (electroporation), Non-cytotoxic nerves/bones regenerating drug delivering agent; Energy Applications: Hydrogen storage, Desalination membrane, Electric insulating flame retarding cable, Solar sell coating materials

Chemical composition

Typical Components: Boron Nitride Nanotubes >90 wt%, Carbon >6 wt%, Magnesium Oxide >2 wt%

Color

White