Phthalonitrile resin PN-3М cured 180°C

Want to keep this datasheet? Save it now in your required format

Description

PN-3M is a single part phthalonitrile resin with higher glass transition temperature and outstanding thermal stability, specially developed for vacuum infusion and RTM technologies. Pre-curing at 180°C allows to remove parts from tool after cooling. Post-curing provides glass transition temperature above 450°C. Moreover, PN-3M does not support combustion. Can be used for high temperature tooling up to 450°C. It shows the following features and properties:


  • One-part resin system
  • Epoxy-like processability
  • Incombustible
  • Decomposition temperature 520°C
  • Low moisture saturation
  • Low softening temperature 80°C
  • This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.34 g/cm³

    Show Material materials with Density of 1.34 g/cm³

    ASTM D792

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    4.8 GPa

    Show Material materials with Elastic modulus of 4.8 GPa

    ASTM D638

    Flexural modulus

    23.0 °C

    4.6 GPa

    Show Material materials with Flexural modulus of 4.6 GPa

    ASTM D790

    Flexural strength

    23.0 °C

    4.6 MPa

    Show Material materials with Flexural strength of 4.6 MPa

    ASTM D790

    Plane-Strain Fracture Toughnes

    23.0 °C

    0.76 MPa·√m

    Show Material materials with Plane-Strain Fracture Toughnes of 0.76 MPa·√m

    ASTM D5045

    Tensile strength

    23.0 °C

    60 MPa

    Show Material materials with Tensile strength of 60 MPa

    ASTM D638

    Strain energy release

    ASTM D5045

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    9E-5 1/K

    Show Material materials with Coefficient of thermal expansion of 9E-5 1/K

    ASTM E831

    Heat deflection temperature

    200 °C

    Show Material materials with Heat deflection temperature of 200 °C

    ASTM E2092

    Vicat softening temperature

    80 °C

    Show Material materials with Vicat softening temperature of 80 °C

    Magnetic

    PropertyValue

    Curie temperature

    180 °C

    Show Material materials with Curie temperature of 180 °C

    Technological properties

    Property
    Application areas

    Structures requiring high heat resistance;Parts requiring non-combustibility;Parts of engines and other special applications;High temperature tooling for thermoplastics

    Processing methods

    Assemble the vacuum bag. Perform a leak test, the rate of the vacuum drop should not be more than 1 mbar per minute. The residual pressure in the bag must not be more than 10 mbar. Assemble the second vacuum bag, put airweave material between the layers of the vacuum film. Perform a leak test for the second vacuum bag. The residual pressure in the bag must not be more than 10 mbar. Degas for 30-40 minutes, at 150-160°C, at a pressure of no more than 10 mbar. During the degassing, the resin should be stirred intensively. Heat the tool up to 150-170°C. Maintaining the temperature of resin dispenser at 160°C, start the infusion process. After complete impregnation of the bag, close the resin inputs, but continue evacuation from the inner bag for at least 30 minutes. Then close the outputs from the inner bag. Maintain the outer vacuum bag until the end of curing process. Increase the temperature at a rate of 2°C/min to 180°C. Dwell at 180°C for 6 hours. Before removing the part, cool the mold to at least 60°C at a speed of no more than 5°C/min. Post-cure can be performed without tooling. Heat to 180°C at a rate of 2°C/min, then heat to 375°C at a rate of 5-10°C/min. Dwell at 375°C for 8 hours. Cool down the part to 60°C at rate <5°C/min. For the measurement of vacuum, the use of absolute pressure sensors is recommended.