Epoxy resin TK123

Want to keep this datasheet? Save it now in your required format

Description

TK123 is a two-part low viscosity epoxy infusion resin developed for tooling up to 120°С, or CFRP parts with sustainable properties up to 90°С. The resin offers simple and flexible processing due to low viscosity at room temperature (lower than 500 mPa*s at 25°C). TK123 was developed specially for vacuum infusion molding, to produce laminates with low porosity and good mechanical performance. It shows the following features and properties:


  • Two-part resin system for vacuum infusion and RTM
  • Wide processing window > 2 hours at 25°C
  • Curing at room temperature
  • Low exotherm
  • High mechanical properties
  • For tooling up to 120°C
  • This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.14 g/cm³

    Show Material materials with Density of 1.14 g/cm³

    ASTM D792

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    3.56 GPa

    Show Material materials with Elastic modulus of 3.56 GPa

    ASTM D638

    Flexural strength

    23.0 °C

    161 MPa

    Show Material materials with Flexural strength of 161 MPa

    ASTM D790

    Plane-Strain Fracture Toughnes

    23.0 °C

    0.96 MPa·√m

    Show Material materials with Plane-Strain Fracture Toughnes of 0.96 MPa·√m

    ASTM D5045

    Tensile strength

    23.0 °C

    80 MPa

    Show Material materials with Tensile strength of 80 MPa

    ASTM D638

    Strain energy release

    ASTM D5045

    Thermal

    PropertyValueComment

    Glass transition temperature

    101 °C

    Show Material materials with Glass transition temperature of 101 °C

    ASTM E2092

    Technological properties

    Property
    Application areas

    Marine: The shells of boats and sport catamarans can be made of composites;Composite tooling: ITECMA composite tooling materials combines low CTE index with extreme lightness.

    Processing methods

    Thoroughly mix components A and B at 25°C in a 1: 0.434 weight ratio. The error in the dosage of components should not exceed 2%. Particular attention should be given to mixing at the walls and bottom of the mixing tank. It is recommended to use devices with automatic mixing and mix under vacuum. Degas the resin with intensive mixing for 15-30 minutes at 20-25°С, pressure no more than 10 mbar. Assemble vacuum bag. Perform a leak test, the rate of the vacuum loss should not be more than 1 mbar per minute. The residual pressure in the bag must not be more than 10 mbar. Assemble the second vacuum bag, between the layers of the vacuum film airweave should be laid . Carry out a leak test of the second vacuum bag. The residual pressure in the bag must not be more than 10 mbar. Maintain temperature at 25-40°C. The recommended impregnation temperature is 25-35°C. It is recommended to preliminarily dry the reinforcing material in vacuum bag at 60-80°C for at least 1 hour. Maintaining the temperature of the mold at 25-35°C, start the infusion process. After complete impregnation, close the resin inputs, continue evacuation from inner bag for at least 30 minutes at 25-40°C. Close the outputs from the inner bag. Continue evacuation from outer vacuum bag until gelation (~24h at 25°C). After 48-72 hours, you can remove the part from the mold and post-cure without mold. Post-cure: Increase the temperature at a rate of 2°C/h to 80°C, keep it at 80°C for 6 hours. Curing is allowed immediately after the impregnation process without being removed from the mold. Increase the temperature at a rate of 2°C/min to 80°C, exposure at 80°C for 6 hours. Before removing the part, cool the tooling to at least 50°C at a speed of no more than 5°C/min. Curing (heating rate 2°C/min) or post-curing (heating rate 2°C/h) to 120°C is permissible to obtain a glass transition temperature of 140°C.