Description

T107 is a prepreg based on epoxy resin and reinforcing filler (unidirectional tapes or fabrics of various weaving) for producing details with operating temperatures up to 150°C. It shows the following features and properties:


  • High strength
  • High impact- and cracking-resistance
  • Glass-transition temperature is 175°C
  • This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Water absorption

    23.0 °C

    3.57 %

    Show Material materials with Water absorption of 3.57 %

    for 54h to boiling water

    Mechanical

    PropertyTemperatureValueComment

    Flexural strength

    23.0 °C

    189 MPa

    Show Material materials with Flexural strength of 189 MPa

    ASTM D790

    Plane-Strain Fracture Toughnes

    23.0 °C

    2.08 MPa·√m

    Show Material materials with Plane-Strain Fracture Toughnes of 2.08 MPa·√m

    ASTM D5045

    Tensile strength

    23.0 °C

    82 MPa

    Show Material materials with Tensile strength of 82 MPa

    ASTM D638

    Strain energy release

    ASTM D5045

    Thermal

    PropertyValueComment

    Glass transition temperature

    175 °C

    Show Material materials with Glass transition temperature of 175 °C

    ASTM E2092

    Technological properties

    Property
    Application areas

    High-loaded automotive parts;Sports equipment: Bicycle, frame, wheels, seat, seat post, handlebar, head stem and crank arm of a sports bicycle are made of carbon composite;Geometry strengthen elements: Experimental stringer panel;High-loaded aircraft parts: Aircraft engine hoods

    Processing methods

    Heating 2°С/min in 1 bar pressure up to 150°С. Then expose it for 30 min. Heating again at 2°С/min in 2 bar pressure up to 150°С. Then expose it for 180 min and pressure 3-6 bar. Last step is cooling with 5°С/min to 50°С.