General
Property | Value | Shape |
---|---|---|
Density | 4.51 g/cm³ Show Material materials with Density of 4.51 g/cm³ | Sheet, Plate |
Dimension
Property | Value | Shape |
---|---|---|
Length | 1500 mm Show Material materials with Length of 1500 mm | Sheet, Plate |
5000 mm Show Material materials with Length of 5000 mm | Sheet | |
6500 mm Show Material materials with Length of 6500 mm | Plate | |
Width | 400 mm Show Material materials with Width of 400 mm | Sheet |
600 mm Show Material materials with Width of 600 mm | Plate | |
1524 mm Show Material materials with Width of 1524 mm | Sheet | |
1600 mm Show Material materials with Width of 1600 mm | Plate |
valueMetaData
Property | Value |
---|
Mechanical
Property | Value | Shape | Comment |
---|---|---|---|
Elastic modulus | 106.0 GPa Show Material materials with Elastic modulus of 106.0 GPa | Sheet, Plate | |
Hardness, Brinell | 200.0 Show Material materials with Hardness, Brinell of 200.0 | Sheet, Plate | |
Poisson's ratio | 0.361 [-] Show Material materials with Poisson's ratio of 0.361 [-] | Typical for Pure Titanium | |
Shear modulus | 46.0 GPa Show Material materials with Shear modulus of 46.0 GPa | Typical for Pure Titanium | |
Tensile strength | 550.0 MPa Show Material materials with Tensile strength of 550.0 MPa | Sheet, Plate | |
Yield strength | 485.0 MPa Show Material materials with Yield strength of 485.0 MPa | Sheet, Plate |
Thermal
Property | Value | Shape | Comment |
---|---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | |
Melting point | 1670.0 °C Show Material materials with Melting point of 1670.0 °C | Typical for Pure Titanium | |
Specific heat capacity | 540 J/(kg·K) Show Material materials with Specific heat capacity of 540 J/(kg·K) | Sheet, Plate | |
Thermal conductivity | 18 W/(m·K) Show Material materials with Thermal conductivity of 18 W/(m·K) | Sheet, Plate |
Chemical properties
Property | Value | Shape |
---|---|---|
Carbon | 0.08 Show Material materials with Carbon of 0.08 | Sheet, Plate |
Hydrogen | 0.015 Show Material materials with Hydrogen of 0.015 | Sheet, Plate |
Iron | 0.5 Show Material materials with Iron of 0.5 | Sheet, Plate |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | Sheet, Plate |
Oxygen | 0.4 Show Material materials with Oxygen of 0.4 | Sheet, Plate |