General
Property | Value | Related Standards | Shape |
---|---|---|---|
Density | 4.5 g/cm³ Show Material materials with Density of 4.5 g/cm³ | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Dimension
Property | Value | Related Standards | Shape |
---|---|---|---|
Length | 1500 mm Show Material materials with Length of 1500 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
5000 mm Show Material materials with Length of 5000 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet | |
6500 mm Show Material materials with Length of 6500 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Plate | |
Width | 400 mm Show Material materials with Width of 400 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet |
600 mm Show Material materials with Width of 600 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Plate | |
1524 mm Show Material materials with Width of 1524 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet | |
1600 mm Show Material materials with Width of 1600 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Plate |
valueMetaData
Property | Value |
---|
Mechanical
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastic modulus | 108.0 GPa Show Material materials with Elastic modulus of 108.0 GPa | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Hardness, Brinell | 150.0 Show Material materials with Hardness, Brinell of 150.0 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Poisson's ratio | 0.361 [-] Show Material materials with Poisson's ratio of 0.361 [-] | Typical for Pure Titanium | ||
Shear modulus | 46.0 GPa Show Material materials with Shear modulus of 46.0 GPa | Typical for Pure Titanium | ||
Tensile strength | 345.0 MPa Show Material materials with Tensile strength of 345.0 MPa | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Yield strength | 275.0 MPa Show Material materials with Yield strength of 275.0 MPa | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Thermal
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||
Melting point | 1670.0 °C Show Material materials with Melting point of 1670.0 °C | Typical for Pure Titanium | ||
Specific heat capacity | 520 J/(kg·K) Show Material materials with Specific heat capacity of 520 J/(kg·K) | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Thermal conductivity | 17 W/(m·K) Show Material materials with Thermal conductivity of 17 W/(m·K) | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Carbon | 0.08 Show Material materials with Carbon of 0.08 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Hydrogen | 0.015 Show Material materials with Hydrogen of 0.015 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Iron | 0.3 Show Material materials with Iron of 0.3 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Nitrogen | 0.03 Show Material materials with Nitrogen of 0.03 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Oxygen | 0.25 Show Material materials with Oxygen of 0.25 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Palladium | 0.12 - 0.25 % Show Material materials with Palladium of 0.12 - 0.25 % | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |