Want to keep this datasheet? Save it now in your required format

Description

This UNS R53400 alloy is similar to Titanium Grades 2 and 3 except that UNS R53400 has 0.3% molybdenum and 0.8% nickel. This alloy also offers enhanced corrosion resistance.

Equivalent Materials

This material data has been provided by VSMPO,Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueShape

Density

4.5 g/cm³

Show Material materials with Density of 4.5 g/cm³

Sheet, Plate

Dimension

PropertyValueShape

Length

1500 mm

Show Material materials with Length of 1500 mm

Sheet, Plate

5000 mm

Show Material materials with Length of 5000 mm

Sheet

6500 mm

Show Material materials with Length of 6500 mm

Plate

Width

400 mm

Show Material materials with Width of 400 mm

Sheet

600 mm

Show Material materials with Width of 600 mm

Plate

1524 mm

Show Material materials with Width of 1524 mm

Sheet

1600 mm

Show Material materials with Width of 1600 mm

Plate

valueMetaData

PropertyValue

Mechanical

PropertyValueShape

Elastic modulus

105.0 GPa

Show Material materials with Elastic modulus of 105.0 GPa

Sheet, Plate

Hardness, Brinell

170.0

Show Material materials with Hardness, Brinell of 170.0

Sheet, Plate

Tensile strength

480.0 MPa

Show Material materials with Tensile strength of 480.0 MPa

Sheet, Plate

Yield strength

345.0 MPa

Show Material materials with Yield strength of 345.0 MPa

Sheet, Plate

Thermal

PropertyValueShapeComment

Coefficient of thermal expansion

7.599999999999997e-06 - 1.1e-05 1/K

Show Material materials with Coefficient of thermal expansion of 7.599999999999997e-06 - 1.1e-05 1/K

Typical for Titanium Near Alpha Alloy

Melting point

1540.0 - 1715.0 °C

Show Material materials with Melting point of 1540.0 - 1715.0 °C

Typical for Titanium Near Alpha Alloy

Specific heat capacity

520 J/(kg·K)

Show Material materials with Specific heat capacity of 520 J/(kg·K)

Sheet, Plate

Thermal conductivity

22.6 W/(m·K)

Show Material materials with Thermal conductivity of 22.6 W/(m·K)

Sheet, Plate

Chemical properties

PropertyValueShape

Carbon

0.08

Show Material materials with Carbon of 0.08

Sheet, Plate

Hydrogen

0.015

Show Material materials with Hydrogen of 0.015

Sheet, Plate

Iron

0.3

Show Material materials with Iron of 0.3

Sheet, Plate

Molybdenum

0.2 - 0.4 %

Show Material materials with Molybdenum of 0.2 - 0.4 %

Sheet, Plate

Nickel

0.6 - 0.9 %

Show Material materials with Nickel of 0.6 - 0.9 %

Sheet, Plate

Nitrogen

0.03

Show Material materials with Nitrogen of 0.03

Sheet, Plate

Oxygen

0.25

Show Material materials with Oxygen of 0.25

Sheet, Plate

Looking for suppliers of this material? Click to see 9 supplier of UNS R53400 on Matmatch