General
Property | Value | Shape |
---|---|---|
Density | 4.55 g/cm³ Show Material materials with Density of 4.55 g/cm³ | Bar |
Dimension
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Diameter | 7 mm Show Material materials with Diameter of 7 mm | Bar | ||
115 mm Show Material materials with Diameter of 115 mm | Bar | |||
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Length | 6000 mm Show Material materials with Length of 6000 mm | Bar | max |
Mechanical
Property | Value | Shape | Comment |
---|---|---|---|
Elastic modulus | 100.0 - 120.0 GPa Show Material materials with Elastic modulus of 100.0 - 120.0 GPa | Typical for Titanium Alpha Alloy | |
Elongation | 8.0 - 11.0 % Show Material materials with Elongation of 8.0 - 11.0 % | Bar | |
Tensile strength | 635.0 - 885.0 MPa Show Material materials with Tensile strength of 635.0 - 885.0 MPa | Bar |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 7.599999999999997e-06 - 1.1e-05 1/K Show Material materials with Coefficient of thermal expansion of 7.599999999999997e-06 - 1.1e-05 1/K | Typical for Titanium Alpha Alloy |
Melting point | 1540.0 - 1715.0 °C Show Material materials with Melting point of 1540.0 - 1715.0 °C | Typical for Titanium Alpha Alloy |
Specific heat capacity | 460.0 - 527.0 J/(kg·K) Show Material materials with Specific heat capacity of 460.0 - 527.0 J/(kg·K) | Typical for Titanium Alpha Alloy |
Thermal conductivity | 4.0 - 17.0 W/(m·K) Show Material materials with Thermal conductivity of 4.0 - 17.0 W/(m·K) | Typical for Titanium Alpha Alloy |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminium | 3.5 - 5.0 % Show Material materials with Aluminium of 3.5 - 5.0 % | Bar |
Carbon | 0.1 Show Material materials with Carbon of 0.1 | Bar |
Hydrogen | 0.012 Show Material materials with Hydrogen of 0.012 | Bar |
Iron | 0.3 Show Material materials with Iron of 0.3 | Bar |
Manganese | 0.8 - 2.0 % Show Material materials with Manganese of 0.8 - 2.0 % | Bar |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | Bar |
Oxygen | 0.15 Show Material materials with Oxygen of 0.15 | Bar |
Silicon | 0.12 Show Material materials with Silicon of 0.12 | Bar |
Zirconium | 0.3 Show Material materials with Zirconium of 0.3 | Bar |