Billets with the diameter from 5.12 up to 13.78 inch are produced as saleable products. There are also billets for production of forgings, tubes (tubular billets), bars and shapes. Billets over 13.78 inches in diameter are supplied based on customer requirements. Billets can be made both from Russian and foreign titanium and heat resistant alloys.

Related Standards

Equivalent Materials

This material data has been provided by AluKey,VSMPO,Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueShapeRelated Standards

Density

4.59 g/cm³

Show Material materials with Density of 4.59 g/cm³

Bar, Billet

4.6 g/cm³

Show Material materials with Density of 4.6 g/cm³

DIN 17851

Dimension

PropertyTemperatureValueShapeComment

Diameter

7 mm

Show Material materials with Diameter of 7 mm

Bar

115 mm

Show Material materials with Diameter of 115 mm

Bar

130 mm

Show Material materials with Diameter of 130 mm

Billet

350 mm

Show Material materials with Diameter of 350 mm

Billet

Dimensions

15-65 mm diameter up to 6000 mm length °C

7-14.5 mm diameter up to 3000 mm length

Bar

Length

3000 mm

Show Material materials with Length of 3000 mm

Billet

4500 mm

Show Material materials with Length of 4500 mm

Billet

6000 mm

Show Material materials with Length of 6000 mm

Bar

max

Mechanical

PropertyTemperatureValueShapeRelated StandardsComment

Elastic modulus

114.0 GPa

Show Material materials with Elastic modulus of 114.0 GPa

Bar

117.0 GPa

Show Material materials with Elastic modulus of 117.0 GPa

DIN 17851

Elongation

12.0 %

Show Material materials with Elongation of 12.0 %

Bar, Billet

Hardness, Brinell

350.0 [-]

Show Material materials with Hardness, Brinell of 350.0 [-]

DIN 17851

Reduction of area

20.0 %

Show Material materials with Reduction of area of 20.0 %

DIN 17851

20.0 %

Show Material materials with Reduction of area of 20.0 %

DIN 17851

Transverse

Tensile strength

1000.0 MPa

Show Material materials with Tensile strength of 1000.0 MPa

DIN 17851

1050.0 MPa

Show Material materials with Tensile strength of 1050.0 MPa

DIN 17851

1100.0 MPa

Show Material materials with Tensile strength of 1100.0 MPa

DIN 17851

1138.0 MPa

Show Material materials with Tensile strength of 1138.0 MPa

Bar, Billet

500 °C

750.0 MPa

Show Material materials with Tensile strength of 750.0 MPa

DIN 17851

Yield strength

870.0 MPa

Show Material materials with Yield strength of 870.0 MPa

DIN 17851

RP02

920.0 MPa

Show Material materials with Yield strength of 920.0 MPa

DIN 17851

RP02

960.0 MPa

Show Material materials with Yield strength of 960.0 MPa

DIN 17851

RP02

1035.0 MPa

Show Material materials with Yield strength of 1035.0 MPa

Bar

1050.0 MPa

Show Material materials with Yield strength of 1050.0 MPa

DIN 17851

RP02

Thermal

PropertyTemperatureValueRelated StandardsShapeComment

Coefficient of thermal expansion

20 °C

8.599999999999999e-06 1/K

Show Material materials with Coefficient of thermal expansion of 8.599999999999999e-06 1/K

DIN 17851

200 °C

8.599999999999999e-06 1/K

Show Material materials with Coefficient of thermal expansion of 8.599999999999999e-06 1/K

DIN 17851

Melting point

1500.0 - 1750.0 °C

Show Material materials with Melting point of 1500.0 - 1750.0 °C

Typical for Titanium Alpha Beta Alloy

Specific heat capacity

370.0 - 674.0 J/(kg·K)

Show Material materials with Specific heat capacity of 370.0 - 674.0 J/(kg·K)

Typical for Titanium Alpha Beta Alloy

Thermal conductivity

7.54 W/(m·K)

Show Material materials with Thermal conductivity of 7.54 W/(m·K)

DIN 17851

7.6 W/(m·K)

Show Material materials with Thermal conductivity of 7.6 W/(m·K)

Bar

Electrical

PropertyValueRelated Standards

Electrical resistivity

1.5e-06

Show Material materials with Electrical resistivity of 1.5e-06

DIN 17851

Chemical properties

PropertyValueRelated StandardsShape

Aluminium

3.0 - 5.0 %

Show Material materials with Aluminium of 3.0 - 5.0 %

DIN 17851

Bar, Billet

Carbon

0.08 %

Show Material materials with Carbon of 0.08 %

DIN 17851

Hydrogen

0.0125 %

Show Material materials with Hydrogen of 0.0125 %

Bar, Billet

0.015 %

Show Material materials with Hydrogen of 0.015 %

DIN 17851

Iron

0.20 %

Show Material materials with Iron of 0.20 %

DIN 17851

0.2 %

Show Material materials with Iron of 0.2 %

Bar, Billet

Molybdenum

3.0 - 5.0 %

Show Material materials with Molybdenum of 3.0 - 5.0 %

DIN 17851

Bar, Billet

Nitrogen

0.05 %

Show Material materials with Nitrogen of 0.05 %

DIN 17851

Bar, Billet

Oxygen

0.25 %

Show Material materials with Oxygen of 0.25 %

DIN 17851

0.27 %

Show Material materials with Oxygen of 0.27 %

Bar, Billet

Silicon

0.3 - 0.7 %

Show Material materials with Silicon of 0.3 - 0.7 %

DIN 17851

Bar, Billet

Tin

1.5 - 2.5 %

Show Material materials with Tin of 1.5 - 2.5 %

DIN 17851

Bar, Billet